MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Ineos J60-800-178 HDPE
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Injection Molded

Material Notes: A high density polyethylene homopolymer. It has a narrow molecular weight distribution and is intended for the injection molding of screw caps dedicated to the packaging of still and sparkling water. Parts fabricated from this material exhibit a glossy surface finish, and have good impact strength and rigidity. This material meets the Food and Drug Administration requirements of 21CFR 177.1520.

Key Words: Narrow molecular weight distribution, excellent gloss and rigidity
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.961 g/ccASTM D4883
Environmental Stress Crack Resistance 3.0 hourCond. B, 10%; ASTM D 1693
Melt Flow 8.5 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 65ASTM D2240
Tensile Strength, Yield 31.0 MPa2 in/min.; ASTM D638
Elongation at Break 600 %2 in/min.; ASTM D638
Flexural Modulus 1.552 GPaTangent-Method 1; ASTM D790
Izod Impact, Notched 0.530 J/cmASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 87.0 °CASTM D648
Vicat Softening Point 128 °CASTM D1525
Brittleness Temperature <= -75.0 °CASTM D 746
 
Compliance PropertiesOriginal ValueComments
FDA Yes
 
Descriptive Properties
ProcessInjection

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Ineos T60-800 HDPE
Ineos J50-1000-178 HDPE
Ineos J50-2000-119 HDPE
Ineos J50-1000-187 HDPE
Ineos J60-1700-183 HDPE

PSOLKM002 / 68233

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.