MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Epoxy Technology EPO-TEK® 314 Thermally and Electrically Insulating Epoxy
Categories: Polymer; Thermoset; Epoxy

Material Notes: Material Description: A two component, high temperature grade, thermally and electrically insulating epoxy, designed for adhesive and sealing applications found in semiconductor, electro-optics, fiber optics, medical, and scientific/OEM industries. It is a low viscosity, optical grade epoxy with low index of refraction (Nd).

Information Provided by Epoxy Technology

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.18 g/ccPart A
 1.23 g/ccPart B
Viscosity 300 - 600 cP
@Temperature 23.0 °C
100 rpm
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 83
Tensile Modulus 275210 psiStorage
Shear Strength >= 5100 psiDie
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+13 ohm-cm
Dielectric Constant 3.25
@Frequency 1000 Hz
Dissipation Factor 0.0131
@Frequency 1000 Hz
 
Thermal PropertiesOriginal ValueComments
CTE, linear 39.0 µm/m-°CBelow Tg
 134 µm/m-°CAbove Tg
Maximum Service Temperature, Air 200 °CContinuous
 300 °CIntermittent
Minimum Service Temperature, Air -55.0 °CContinuous
 -55.0 °CIntermittent
Glass Transition Temp, Tg >= 75.0 °CDynamic Cure 20—200°C /ISO 25 Min; Ramp 10—200°C @ 20°C/Min
Decomposition Temperature 361 °CDegradation Temperature
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.4965
@Wavelength 589 nm
uncured
Transmission, Visible >= 96 %
@Wavelength 440 - 1680 nm
Spectral
 
Processing PropertiesOriginal ValueComments
Cure Time 3.00 hour
@Temperature 120 °C
 30.0 min
@Temperature 180 °C
Pot Life 5760 min
Shelf Life 12.0 Month
@Temperature 25.0 °C
 
Descriptive Properties
ColorClear/ColorlessPart A
ConsistencyPourable liquid
Mix Ratio by Weight10:0.6
Number of ComponentsTwo
Weight Loss0.18%200°C
 0.43%250°C
 1.03%300°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Epoxy Technology EPO-TEK® 310M-T Flexible Epoxy
Resinlab® RC8080 Anaerobic Retaining Compound
Resinlab® RC8020 Anaerobic Retaining Compound
Resin Technology Group EN 239-2 Cationic UV Cure Epoxy Adhesive
Resin Technology Group DP031199-1 Cationic UV Cure Epoxy Adhesive

PPOXYT114 / 141153

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.