MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Traid Villarroya TRAIDAMID® E Nylon 6, Extruded
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Extruded

Material Notes:
  • Very abrasion resistant
  • Electrically insulating
  • Good chemical resistance to many oils, diesel, petrol and greases
  • Tough and rigid
  • Easy machined
Industry Applications:
  • Impact and damping plates
  • Conveyor screws
  • Friction bearings
  • Castors
  • Gear wheels

Information provided by Traid Villarroya Hnos. S.L.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.13 g/cc
Water Absorption 3.0 %
@Time 86400 sec
DIN EN ISO 62
 
Mechanical PropertiesOriginal ValueComments
Ball Indentation Hardness 160 MPaISO 2039-1
Tensile Strength, Yield 85.0 MPa50 mm/min; DIN EN ISO 527-2
Elongation at Break 70 %50 mm/min; DIN EN ISO 527-2
Creep Strength 45.0 MPa
@Time 3.60e+6 sec
with static load
Modulus of Elasticity 3.00 GPa1 mm/min; DIN EN ISO 527-2
Charpy Impact Unnotched NBMax. 7,5j; DIN EN ISO 179-1EU
Coefficient of Friction 0.38 - 0.45Against steel p=0,05 N/mm2
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+13 ohm-cmDIN IEC 60093
Surface Resistance 1.00e+12 ohmDIN IEC 60093
Dielectric Constant 3.7 - 7.0
@Frequency 100000 Hz
DIN 53483
Dielectric Strength 20.0 - 50.0 kV/mm
@Thickness 1.00 mm
ASTM 149
Dielectric Loss Index 0.031 - 0.30
@Frequency 100000 Hz
DIN 53483
Comparative Tracking Index 600 VDIN 53480
 
Thermal PropertiesOriginal ValueComments
CTE, linear 80.0 µm/m-°CDIN 53483
Specific Heat Capacity 1.70 J/g-°CISO 22007-4:2008
Thermal Conductivity 0.230 W/m-KISO 22007-4:2008
Melting Point 220 °CDIN 53765
Maximum Service Temperature, Air 100 °CLong term
 160 °CShort term
Glass Transition Temp, Tg 60.0 °CDIN 53765
Flammability, UL94 HBDIN IEC 60995-11-10
 
Descriptive Properties
ColorNatural opaque
Resistance to hot mater / basesLimited
Resistance to weatheringNot resistant
Time yield limit for 1% elong4.5 MPaAfter 1000 hours

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PTRAID900 / 318861

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.