MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Lanxess Addolink® THPE PL Additive/Polycarbonate
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Product Information: Addolink THPE is used for the production of branched polycarbonates and suitable for both common production processes - the interfacial and the melt process. In the case of the interfacial process Addolink THPE can be added together with the bisphenol and other reaction components to the aqueous phase. It is also possible to add Addolink THPE dissolved in the organic solvent. With the melt process Addolink THPE can directly be added at the beginning of the process when the reaction components are melted. However, it can be advantageous if the branching agent is still added at the oligocarbonate stage before the final production of the higher-molecular weight polycarbonate. With Addolink THPE branched polycarbonates with a pronounced pseudoplastic behavior can be obtained. For example branched polycarbonates can favorable be used for the production of large hollow bodies by the extrusion blow molding or injection stretch blow molding process (improved stability under load of the parison) or for the production of twin-wall sheets and profiles with single-screw extruders. In contrast with other branching agents Addolink THPE is almost completely built into the polymer matrix and does not give noticeable discolorations of the end product even after repeated extrusions. Even with small amounts of Addolink THPE (approx. 0.2 - 0.5% related to the bisphenol component) branched polycarbonates with a pronounced pseudoplastic behavior are obtained.

Function: Production of branched polycarbonates

Information provided by Lanxess.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.226 g/cc0.04429 lb/in³
Water Absorption <= 0.20 %<= 0.20 %
 
Thermal PropertiesMetricEnglishComments
Melting Point 245 - 248 °C473 - 478 °F
 
Processing PropertiesMetricEnglishComments
Shelf Life 24.0 Month24.0 Month
 
Descriptive Properties
Appearancewhite powder
Specifications>99.5%Purity
 0.051 g/lSolubility in water

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PLANY8212 / 208605

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.