MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Polykemi AB POLYfill PP CIP6015F VTUV Polypropylene, Mineral Reinforced, Heat and UV Stabilized
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with 20% Talc Filler

Material Notes:

Information provided by Polykemi AB

Key Words: Polypropylene
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.00 g/cc0.0361 lb/in³ISO 1183
Filler Content 15 %15 %±2%; Polykemi
Linear Mold Shrinkage, Flow 0.0090 - 0.011 cm/cm0.0090 - 0.011 in/inISO 2577
Linear Mold Shrinkage, Transverse 0.0090 - 0.011 cm/cm0.0090 - 0.011 in/inISO 2577
Melt Index of Compound 15 g/10 min
@Load 2.16 kg,
Temperature 230 °C
15 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break <= 24.0 MPa<= 3480 psiISO/R527
Elongation at Break 55 %55 %ISO/R527
Elongation at Yield 7.0 %7.0 %ISO/R527
Flexural Strength <= 37.0 MPa<= 5370 psiISO 178
Flexural Modulus 1.80 GPa
@Temperature 23.0 °C
261 ksi
@Temperature 73.4 °F
ISO 178
Charpy Impact Unnotched  NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ISO 179
 NB
@Temperature -20.0 °C
NB
@Temperature -4.00 °F
ISO 179
Charpy Impact, Notched  0.400 J/cm²
@Temperature -30.0 °C
1.90 ft-lb/in²
@Temperature -22.0 °F
ISO 179
 2.00 J/cm²
@Temperature 23.0 °C
9.52 ft-lb/in²
@Temperature 73.4 °F
ISO 179
 
Thermal PropertiesMetricEnglishComments
CTE, linear 60.0 - 80.0 µm/m-°C33.3 - 44.4 µin/in-°FPolykemi
Deflection Temperature at 0.46 MPa (66 psi) 123 °C253 °F120°C/h; ISO 75/1
Deflection Temperature at 1.8 MPa (264 psi) 66.0 °C151 °F120°C/h; ISO 75/1
Vicat Softening Point  63.0 °C
@Load 5.001 kg
145 °F
@Load 11.03 lb
50°C/h; ISO 306
 139 °C
@Load 1.00 kg
282 °F
@Load 2.21 lb
50°C/h; ISO 306
 
Processing PropertiesMetricEnglishComments
Melt Temperature 230 - 260 °C446 - 500 °F
Mold Temperature 60.0 - 80.0 °C140 - 176 °F
Drying Temperature 70.0 - 80.0 °C158 - 176 °F
Dry Time 2 - 4 hour2 - 4 hourin circulation dryer
 2 - 4 hour2 - 4 hourin desiccant air dryer
Injection Pressure 40.0 - 70.0 MPa5800 - 10200 psi
Back Pressure 0.500 - 1.50 MPa72.5 - 218 psi
 
Descriptive Properties
Holding Pressure< 20% of injection pressure
Injection SpeedMedium
Scratch Resistance, 10N (dL)0.1210N Fine Structure; ISO 1518/D65

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
RTP Company RTP 199 X 134954 A Polypropylene (PP) Mineral - Flame Retardant - Non-PBB/PBDE - UV Resistant
Multibase Multi-Pro® 2005 XRC Black 20% Filler Content Polypropylene
LATI Latene® EP 22UVH2 MX/25 PP Copolymer, Mineral Reinforced
Buckeye Polymers BP RPP 2011 C Polypropylene, 20% Mineral Filled
Buckeye Polymers BP RPP 2008 T NAT Polypropylene, Talc Filled

PPOLYK248 / 122973

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.