MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
PoolKemie RESINPOL R 601 Polyester resin
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Description: Styrene-dissolved, thixotropic, pre-accelerated, orthoophthalic acid based polyester resin. Excellent impregnation features and mechanical characteristics.

Application: It is designed for the most critical applications for a thermosetting resin. Resin R 601 is suitable for the production of car parts, shipbuilding, helmets, industrial parts and all other products requiring high resistance.

Information provided by Poolkemie

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.00 - 1.20 g/ccSystem Characteristics
 1.10 - 1.30 g/ccCured
Solids Content 57 - 61 %PK04
Brookfield Viscosity 400 - 700 cP(9.8 sec-1) PK01
 1500 - 2700 cP(0.98 sec-1) PK01
Linear Mold Shrinkage 0.0023 - 0.0029 cm/cmCured
Storage Temperature <= 25.0 °C
 
Mechanical PropertiesOriginal ValueComments
Hardness, Barcol 35 - 41Cured; ASTM-D 2583
Elongation at Break 2.3 - 2.7 %Cured; UNI EN 61
 
Processing PropertiesOriginal ValueComments
Gel Time 8.00 - 14.0 minPK02
Shelf Life 4.00 Month
 
Descriptive Properties
Exothermic peak150-160°CTemperature, PK02
 16-24 mintime, PK02

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PPOOLK059 / 318538

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.