MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Crucible Steel CRUCIBLE A9 Tool Steel
Categories: Metal; Ferrous Metal; Tool Steel; Air-Hardening Steel

Material Notes: Crucible A9 is an air-hardening tool steel combining some of characteristics of the 5% chromium hot-work grades (such as H13) with the high attainable hardness and compressive yield strength of the cold-work grades such as A2). Crucible A9 is suitable for hot and cold work applications requiring high toughness, hardness, or heat check resistance, and moderate wear resistance.

Information provided by Crucible Industries

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.78 g/cc0.281 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 217 - 241217 - 241
Hardness, Rockwell C  47
@Tempering Temp. 593 °C
47
@Tempering Temp. 1100 °F
hardened at 1800°F then tempered
 52.5
@Tempering Temp. 566 °C
52.5
@Tempering Temp. 1050 °F
hardened at 1800°F then tempered
 54.5
@Tempering Temp. 538 °C
54.5
@Tempering Temp. 1000 °F
hardened at 1800°F then tempered
 56
@Tempering Temp. 482 °C
56
@Tempering Temp. 900 °F
hardened at 1800°F then tempered
 56.5
@Tempering Temp. 510 °C
56.5
@Tempering Temp. 950 °F
hardened at 1800°F then tempered
Modulus of Elasticity 207 GPa30000 ksi
Charpy Impact  67.8 J
@Tempering Temp. 482 °C
50.0 ft-lb
@Tempering Temp. 900 °F
hardened at 1800°F then tempered; C-notch
 67.8 J
@Tempering Temp. 510 °C
50.0 ft-lb
@Tempering Temp. 950 °F
hardened at 1800°F then tempered; C-notch
 152 J
@Tempering Temp. 538 °C
112 ft-lb
@Tempering Temp. 1000 °F
hardened at 1800°F then tempered; C-notch
 182 J
@Tempering Temp. 566 °C
134 ft-lb
@Tempering Temp. 1050 °F
hardened at 1800°F then tempered; C-notch
 205 J
@Tempering Temp. 593 °C
151 ft-lb
@Tempering Temp. 1100 °F
hardened at 1800°F then tempered; C-notch
 
Thermal PropertiesMetricEnglishComments
CTE, linear  12.1 µm/m-°C
@Temperature 20.0 - 427 °C
6.70 µin/in-°F
@Temperature 68.0 - 800 °F
 12.4 µm/m-°C
@Temperature 20.0 - 538 °C
6.90 µin/in-°F
@Temperature 68.0 - 1000 °F
 12.6 µm/m-°C
@Temperature 20.0 - 649 °C
7.00 µin/in-°F
@Temperature 68.0 - 1200 °F
Thermal Conductivity 25.8 W/m-K
@Temperature 95.0 °C
179 BTU-in/hr-ft²-°F
@Temperature 203 °F
 
Processing PropertiesMetricEnglishComments
Processing Temperature 804 °C1480 °FCritical Thermal Treatment Temperature
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.50 %0.50 %
Chromium, Cr 5.2 %5.2 %
Iron, Fe 89.2 %89.2 %as balance
Manganese, Mn 0.30 %0.30 %
Molybdenum, Mo 1.4 %1.4 %
Nickel, Ni 1.4 %1.4 %
Silicon, Si 1.0 %1.0 %
Vanadium, V 1.0 %1.0 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Carpenter S7 Alloy Tool Steel (AISI S7)
AISI Type A9 Tool Steel
AISI Type A7 Tool Steel
AISI Type D7 Air-Hardening Cold-Work Tool Steel (UNS T30407)
AISI Type M2 Molybdenum High Speed Tool Steel (UNS T11302)

NCRUC911 / 160362

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.