MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

(Viewing data as-entered. Click here to return)
Rogers Arlon Thermabond® T20 (99710W015) 0.015" (0.381 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier
Categories: Polymer; Thermoset; Silicone; Silicone Rubber; Silicone, Molded, Glass Fiber Filled

Material Notes: Description: 15 mil thick Thermabond® T20 electrically insulating electronic adhesive.

Design/Construction:
Liner: FEP
Product: Uncured Silicone Rubber
Carrier: PTFE Coated Fiberglass

Recommended Primers: Dow Corning S2260 or Lord Chemical Chemlock® 607

Product Use: Thermally conductive, electrically insulating electronic adhesive. Bonds with primer.

Appearance: White, High viscosity gum

This data represents typical values for the production material. The data should not be used to write, or in place of, material specifications.

Information provided by Arlon Silicone Technologies Division; now a part of Rogers Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.30 g/ccSilicone Property; Arlon SQA-TMS-024
Thickness 1.00 milLiner
 3.00 milCarrier
 15.0 milOverall; Arlon SQA-TMS-003
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 83Silicone Property; ASTM D2240
Tensile Strength 650 psiSilicone Property; ASTM D412
Elongation at Break 25 %Silicone Property; ASTM D412
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 1000 V/milASTM D149
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 0.800 W/m-KSilicone Property; ASTM E 1530
 1.33 W/m-KProduct Property; ASTM E 1530
Maximum Service Temperature, Air 400 °F
Minimum Service Temperature, Air -100 °F
Glass Transition Temp, Tg -116 °CSilicone Property; ASTM D1356
 
Processing PropertiesOriginal ValueComments
Cure Time 15.0 min
@Temperature 141 °C
Recommended Cure Cycle
Shelf Life 6.00 Month
@Temperature 4.44 - 10.0 °C
From date of manufacture
 
Descriptive Properties
ColorWhite
Total Product Weight (g/m2)610Arlon SQA-TMS-025

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Shandong Dawn Dawnprene 624-80A TPV (EPDM/PP)
Rubatex R495 EPDM Rubber Foam Sheet
Rogers Arlon Thermabond® T20 (99710W008) 0.008" (0.203 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier
Polykemi AB POLYfill PP EIP8020F Polypropylene/EPDM, Mineral Reinforced
Lucobit Lucobatch® 1850 T20 Polyolefin TPO Granules

PARL489 / 125675

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.