DAI-EL® G-7400BP is a bisphenol curable, gum copolymer. It has excellent mold flow compared with other fluoroelastomers of medium Mooney viscosity, making it well suited for compression, transfer or injection molding. Properly compounded, DAI-EL® G-7400BP produces vulcanizates with excellent heat and compression set resistance. Typical Applications: O-rings, shaft seals, gaskets, molded tubing Rheological Properties MDR 2000: Temperature: 177°C Frequency: 100 cpm Strain: 0.5° Test time: 6 min Rheological Properties ODR: Temperature: 177°C Frequency: 100 cpm Strain: 3 ° Test time: 12 min Information provided by Daikin. |