MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

HB Fuller MP5405 Structural Adhesive
Categories: Polymer; Thermoplastic; Adhesives, Sealants, and Coatings

Material Notes: MP5405 is a two part unfilled epoxy adhesive designed for ceramics, and most plastics. It cures to a tough semi-rigid material, and is a free flowing viscosity. It gives good resistance to water, salt spray, inorganic acids and bases, and most organic solvents. It was especially formulated to a 1:1 mix ratio for use in either MMD equipment or side-by-side dual cartridges for easy dispensing. Handling strength is normally achieved at room temperature within 3-5 minutes with full cure in 24 hours. An elevated temperature cure schedule can be used to reach final properties quickly.

Features and Benefits:

  • Excellent Adhesion Properties
  • Excellent Bonding to Metals, Ceramics and Most Plastics
  • Excellent Chemical Resistance
  • Suitable for Cartridge and MMD Dispensing Equipment
  • Excellent Thermal Performance
  • 100% Reactive
  • Room Temperature Cure
  • 1:1 volume mix product for easy meter or static mix of application

Information provided by H.B. Fuller Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.15 g/cc1.15 g/ccPart B
 1.16 g/cc1.16 g/ccMixed
 1.16 g/cc1.16 g/ccPart A
Viscosity 12000 cP12000 cPPart A
 13000 cP13000 cPPart B
 125000 cP125000 cPMixed
Storage Temperature 12.0 - 25.0 °C53.6 - 77.0 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 8080ASTM D2240
Tensile Strength 48.3 MPa7010 psiASTM D638
Elongation at Break 3.0 - 5.0 %3.0 - 5.0 %ASTM D638
Shear Strength 15.9 MPa2310 psiOverlap Shear Strength, Aluminum, Acid Etched at 25°C; ASTM D1002
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 8.00e+14 ohm-cm8.00e+14 ohm-cmASTM D257
Dielectric Constant 4.5
@Frequency 100 Hz
4.5
@Frequency 100 Hz
ASTM D150
Dielectric Strength 16.1 kV/mm409 kV/inASTM D149
 
Processing PropertiesMetricEnglishComments
Cure Time 3.00 - 5.00 min0.0500 - 0.0833 hourHandling
 1440 min
@Temperature 23.0 °C
24.0 hour
@Temperature 73.4 °F
Pot Life 3.00 - 5.00 min3.00 - 5.00 min
Shelf Life 12.0 Month12.0 Month
 
Descriptive Properties
ColorClear
ConsistencyLiquid
Mix Ratio1:1Volume
 1:1Weight

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PHBFULL189 / 316980

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.