MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Sika Sikasil® 728 RCS Two-part, self-leveling, rapid cure, ultra low modulus, horizontal application, neutral cure silicone sealant
Categories: Polymer; Adhesive; Thermoset; Silicone; Silicone, RTV, Adhesive/Sealant Grade

Material Notes: Sikasil-728 RCS (Rapid Cure System) is a self-leveling, two-component, very rapid cure, ultra low modulus elastomeric, neutral cure silicone sealant. Exceeds the requirements of ASTM C-920, Type M, Grade P, Class 100/50, Use T, M, G, A, O; TT-S-00227E, Type I, and various AASHTO reports and state DOT approvals.

Where to Use: Construction Application:

  • Horizontal expansion joints
  • Highway and bridge joints
  • Saw cut joints - new and remedial
  • Plaza decks
  • Parking decks
  • Bridges
  • Airports
  • Stadiums
  • Driveways
Location:
  • Horizontal
  • Interior and exterior
  • Above grade or on grade
Substrate:
  • Concrete, steel, glass, aluminum, tile, ceramic, masonry, brick, stone and granite
Advantages:
  • No tooling, less labor
  • Excellent flexibility for extreme high and low temperature conditions
  • Excellent flexibility for dynamic joint movement
  • Bonds to most substrates without priming
  • Open to traffic in one hour
  • All season ease of application
  • Good contact/adhesion with hard to reach areas
  • Ideal for cold climates
  • Excellent for use on runways and tarmacs
  • Jet fuel resistant
  • Resistant to road salts

Information provided by Sika Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Volatile Organic Compounds (VOC) Content 30 g/l30 g/l2.4% by wt
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 4.0 - 6.04.0 - 6.0ASTM C-661 & ASTM D-2240
Hardness, Shore OO 45 - 5545 - 55ASTM C-661 & ASTM D-2240
Tensile Strength 0.483 MPa70.0 psiASTM D412
Tensile Stress at Strain 0.172 MPa
@Strain 100 %
25.0 psi
@Strain 100 %
ASTM D412
Elongation at Break 725 %725 %ASTM D412
 >= 1000 %>= 1000 %Joint (a) (b); ASTM D-5329
Tensile Modulus 0.0000345 GPa
@Strain 100 %
0.00500 ksi
@Strain 100 %
Joint (a) (b); ASTM D-5329
Peel Strength 5.26 kN/m30.0 plion aluminum, glass and concrete; ASTM C794
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 177 °C350 °F
Minimum Service Temperature, Air -62.2 °C-80.0 °F
 
Processing PropertiesMetricEnglishComments
Cure Time 10.0 min0.167 hourSkin-over Time
 60.0 min1.00 hour19%
Tack-Free Time 25.0 min0.417 hour
Shelf Life 12.0 Month
@Temperature <=32.0 °C
12.0 Month
@Temperature <=89.6 °F
in original unopened cartridge
 
Descriptive Properties
Colordark grayPart A
 Limestone and Charcoal GrayMixed
 whitePart B

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Silicone, RTV, Adhesive/Sealant Grade

PSIKA951 / 209858

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.