MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

3M SJ5202 Protective Product, Die Cut Shapes
Categories: Polymer; Thermoset; Polyurethane, TS

Material Notes: 3M Bumpon Protective Products SJ5201 and SJ5202 are pressure-sensitive, adhesive backed polyurethane products made from SJ5200 Series soft foam rollstock. A hexagon shape is often preferred for various cushioning stop and non-skid foot applications. These products have a very high tack adhesive system (synthetic rubber, R-25), which has the capability of providing excellent adhesion to a wide variety of substrates. This includes many low surface energy substrates such as polypropylene, polyethylene, and powder coated paints.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.640 g/cc0.0231 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore M 3636ASTM D2240
Peel Strength 9.12 kN/m52.0 pli90°, Adhesion to Polypropylene
 9.64 kN/m55.0 pli90°, Adhesion to Polystyrene
 9.64 kN/m55.0 pli90°, Adhesion to ABS
 9.64 kN/m55.0 pli90°, Adhesion to Stainless Steel
 9.64 kN/m55.0 pli90°, Adhesion to Aluminum
Compression Set >= 10 %
@Temperature 62.0 °C,
Time 79200 sec
>= 10 %
@Temperature 144 °F,
Time 22.0 hour
50% Deflection; ASTM D1056
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 66.0 °C151 °F
 107 °C225 °FIntermittent
Minimum Service Temperature, Air -34.0 °C-29.2 °F
 
Processing PropertiesMetricEnglishComments
Processing Temperature >= 5.00 °C>= 41.0 °FApplication
 <= 52.0 °C<= 126 °FApplication
 
Descriptive Properties
AppearanceLight Brown

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMM35254 / 170001

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.