MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

(Viewing data as-entered. Click here to return)
CHT Group EP RAP 45 14 EPI Engineered Polymers Aliphatic Polyurea
Categories: Polymer; Thermoset; Polyurethane, TS

Material Notes: EP RAP 45 14 Aliphatic Polyurea, “Powered by Reactamine® Technology”, is a two component 100% solids, no VOC’s, aliphatic polyurea coating that was developed for UV stable (colorfast) polyurea flooring applications. This new generation polyurea displays fast cure times and excellent adhesion characteristics. EP RAP 45 14 was designed to be quick gelling (15 minutes) in order to optimize leveling and wetting properties. EP RAP 45 14 can be spray applied at temperatures ranging from 20ºF to 120ºF. This 100% polyurea elastomer displays excellent chemical resistance, water insensitivity and UV resistance (in any color) at a wide range of temperatures. EP RAP 45 14 will provide a smooth glossy finish when fully cured. An aggregate can be broadcast into this self-leveling material to provide a non-skid surface. EP RAP 45 14 emits virtually no odors and can be applied indoors without high VOC levels contributed to most epoxies and polyurethanes. EP RAP 45 14 meets to USDA and FDA specifications.

Applications:

  • AIRCRAFT HANGAR FLOORS
  • LOW TEMPERATURE EQUIPMENT
  • MAINTENANCE FACILITIES
  • FLOORS REQUIRING UV STABILITY
  • UV-STABLE TOP COAT
  • INDUSTRIAL SHOP FLOORS
  • NON-CONDUCTIVE FLOORING
  • Part of the Amber Chemical Group. Data provided by manufacturer.

    Formerly Amber Chemical Co (ACC Silicones), aquired by CHT in 2017

    Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesOriginal ValueComments
    Viscosity 575 cP
    @Temperature 75.0 °C
    B Side
     750 cP
    @Temperature 75.0 °C
    A Side
     
    Mechanical PropertiesOriginal ValueComments
    Hardness, Shore D 40ASTM 2240
    Tensile Strength 3610 psiASTM D412
    Elongation at Break 290 %ASTM D412
    Adhesive Bond Strength >= 250 psiWood (no primer), Delamination; ASTM D4541 Elcometer
     >= 300 psiConcrete (primer), Concrete Failure; ASTM D4541 Elcometer
     >= 300 psiConcrete (epoxy), Concrete Failure; ASTM D4541 Elcometer
     >= 300 psiConcrete (no primer), Concrete Failure; ASTM D4541 Elcometer
     >= 900 psiSteel (no primer), Substrate Failure; ASTM D4541 Elcometer
     >= 1500 psiSteel (epoxy primer), Primer Failure; ASTM D4541 Elcometer
    Tear Strength 480 pliASTM D412
    Taber Abrasion, mg/1000 Cycles 40CS17 Wheel, 1kg; ASTM D4060
     
    Thermal PropertiesOriginal ValueComments
    Flash Point >= 200 °FASTM Pensky-Martin
     
    Processing PropertiesOriginal ValueComments
    Tack-Free Time >= 0.500 hour
    @Temperature 75.0 °C
    Pot Life 40.0 min
    @Temperature 75.0 °C
     
    Compliance PropertiesOriginal ValueComments
    USDA Yes
     
    Descriptive Properties
    ColorAll primary colors.
    Flexibility PassASTM D1737, 1/8"Mandrel
    Resistance to 1,1,1-TrichlorethaneConditional
    Resistance to Acetic Acid (100%)Conditional
    Resistance to AcetoneConditional
    Resistance to Ammonium Hydroxide (50%)Recommended Conditional
    Resistance to Benzene Conditional
    Resistance to Brine-Saturated H2ORecommended Resistance to Brine-Saturated H2O (310g/l)
    Resistance to Chlorinated H2ORecommended
    Resistance to Clorox® (10%) H2ORecommended
    Resistance to Diesel Fuel Recommended Conditional
    Resistance to GasolineRecommended Conditional
    Resistance to Gasoline/ 5% MethanolRecommended Conditional
    Resistance to Gasoline/5% MTBERecommended Conditional
    Resistance to H2ORecommended
    Resistance to H2O (14 days at 82°C)Recommended Conditional
    Resistance to Hydraulic Fluid (oil) Recommended Conditional
    Resistance to Hydrochloric Acid (20%)Recommended
    Resistance to Hydrofluoric Acid(10%)Not Recommended
    Resistance to Isopropyl AlcoholRecommended
    Resistance to Lactic AcidRecommended Conditional
    Resistance to MEKRecommended Conditional
    Resistance to MethanolRecommended
    Resistance to Methylene Chloride Conditional
    Resistance to Mineral Spirits Recommended Conditional
    Resistance to Motor OilRecommended
    Resistance to MTEBConditional
    Resistance to Muriatic Acid (10%)Recommended
    Resistance to NaCl/H2O (10%)Recommended
    Resistance to Nitric Acid (20%)Not Recommended
    Resistance to Phosphoric Acid (10%)Recommended
    Resistance to Phosphoric Acid (50%)Not Recommended
    Resistance to Potassium Hydroxide (10%)Recommended
    Resistance to Potassium Hydroxide (20%)Recommended, Discoloration
    Resistance to Propylene CarbonateRecommended Conditional
    Resistance to Skydrol® Conditional
    Resistance to Sodium BicarbonateRecommended
    Resistance to Sodium Hydroxide (25%)Recommended
    Resistance to Sodium Hydroxide (50%)Recommended, Discoloration
    Resistance to Sodium Hypochlorite (10%)Recommended
    Resistance to Stearic AcidRecommended
    Resistance to Sugar/H2ORecommended
    Resistance to Sulfuric Acid (>50%)Recommended Conditional
    Resistance to Sulfuric Acid (10%)Recommended
    Resistance to TolueneRecommended
    Resistance to Trisodium PhosphateRecommended
    Resistance to Vinegar/ H2O (5%)Recommended
    Resistance to Xylene Recommended Conditional

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

    Users viewing this material also viewed the following:
    CHT Group EP LCP EPI Engineered Polymers Aromatic Polyurea
    CHT Group EP RAP 45 EPI Engineered Polymers Aliphatic Polyurea
    CHT Group EP RAP 60 EPI Engineered Polymers Aliphatic Polyurea
    CHT Group 1KSP EPI Engineered Polymers Silicone Polyurea Dispersion
    CHT Group EP EF EPI Engineered Polymers Extra Flex Polyurea

    PACC109 / 22236

    Metal adhesives

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.