MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Celanese Zytel® 73G15L NC010 PA6-GF15
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 20% Glass Fiber Filled

Material Notes: 15% Glass Reinforced Polyamide 6

Former DuPont product acquired by Celanese in 2022.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.23 g/ccDAM; ISO 1183
Melt Density 1.07 g/cc
@Temperature 270 °C
Water Absorption 7.6 %
@Thickness 2.00 mm
DAM; Sim. to ISO 62
Moisture Absorption 2.50 %
@Thickness 2.00 mm
DAM; Sim. to ISO 62
Viscosity Number 139 cm³/gDAM; ISO 307, 1157, 1628
Linear Mold Shrinkage, Flow 0.0030 cm/cmDAM; ISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.0080 cm/cmDAM; ISO 294-4, 2577
 
Mechanical PropertiesOriginal ValueComments
Ball Indentation Hardness 123 MPaH 961/30; 50% RH; ISO 2039-1
 210 MPaH 961/30; DAM; ISO 2039-1
Tensile Strength at Break 70.0 MPa50% RH; ISO 527-1/-2
 140 MPaDAM; ISO 527-1/-2
Elongation at Break 4.0 %DAM; ISO 527-1/-2
 10 %50% RH; ISO 527-1/-2
Tensile Modulus 3500 MPa50% RH; ISO 527-1/-2
 6000 MPaDAM; ISO 527-1/-2
Flexural Strength 90.0 MPaDS; 50% RH; ISO 178
 190 MPaDS; DAM; ISO 178
Flexural Modulus 3100 MPaDS; 50% RH; ISO 178
 5100 MPaDS; DAM; ISO 178
Poissons Ratio 0.35DAM
 0.3750% RH
Izod Impact, Notched (ISO) 5.00 kJ/m²
@Temperature -40.0 °C
DAM; ISO 180/1A
 5.00 kJ/m²
@Temperature -30.0 °C
DAM; ISO 180/1A
 6.00 kJ/m²
@Temperature 23.0 °C
DAM; ISO 180/1A
 12.0 kJ/m²
@Temperature 23.0 °C
50% RH; ISO 180/1A
Izod Impact, Unnotched (ISO) 40.0 kJ/m²
@Temperature -40.0 °C
DAM; ISO 180/1U
 45.0 kJ/m²
@Temperature 23.0 °C
DAM; ISO 180/1U
Charpy Impact Unnotched 45.0 kJ/m²
@Temperature -30.0 °C
DAM; ISO 179/1eU
 50.0 kJ/m²
@Temperature 23.0 °C
DAM; ISO 179/1eU
 54.0 kJ/m²
@Temperature -30.0 °C
50% RH; ISO 179/1eU
 95.0 kJ/m²
@Temperature 23.0 °C
50% RH; ISO 179/1eU
Charpy Impact, Notched 6.00 kJ/m²
@Temperature -40.0 °C
DAM; ISO 179/1eA
 6.00 kJ/m²
@Temperature -30.0 °C
DAM; ISO 179/1eA
 7.00 kJ/m²
@Temperature 23.0 °C
DAM; ISO 179/1eA
 14.0 kJ/m²
@Temperature -30.0 °C
50% RH; ISO 179/1eA
 15.0 kJ/m²
@Temperature 23.0 °C
50% RH; ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 37.0 µm/m-°CDAM; ISO 11359-1/-2
 15.0 µm/m-°C
@Temperature 55.0 - 160 °C
DAM; ISO 11359-1/-2
 34.0 µm/m-°C
@Temperature -40.0 - 23.0 °C
DAM; ISO 11359-1/-2
CTE, linear, Transverse to Flow 109 µm/m-°CDAM; ISO 11359-1/-2
 80.0 µm/m-°C
@Temperature -40.0 - 23.0 °C
DAM; ISO 11359-1/-2
 100 µm/m-°C
@Temperature 55.0 - 160 °C
DAM; ISO 11359-1/-2
Specific Heat Capacity 2.47 J/g-°C
@Temperature 270 °C
Melt
Thermal Conductivity 0.190 W/m-K
@Temperature 270 °C
Melt
Melting Point 221 °C10°C/min; DAM; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 220 °CDAM; ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 200 °CDAM; ISO 75-1/-2
Vicat Softening Point 215 °C50°C/h, 50N; DAM; ISO 306
Glass Transition Temp, Tg 15.0 °C10°C/min; 50% RH; ISO 11357-1/-2
 55.0 °C10°C/min; DAM; ISO 11357-1/-2
Flammability, UL94 HB
@Thickness 1.50 mm
DAM; IEC 60695-11-10
 HB
@Thickness 1.50 mm
DAM; IEC 60695-11-10
Flame Spread 25.0 mm/min
@Thickness 1.00 mm
DS; ISO 3795 (FMVSS 302)
Oxygen Index 21 %DAM; ISO 4589-1/-2
 
Processing PropertiesOriginal ValueComments
Melt Temperature 270 °COptimum, Injection
 260 - 280 °CRange, Injection
Mold Temperature 70.0 - 120 °CInjection
 100 °COptimum, Injection
Drying Temperature 80.0 °CInjection
Dry Time 2.00 - 4.00 hourInjection, Dehumidified Dryer
Moisture Content <= 0.20 %Injection
Hold Pressure 50.0 - 100 MPaRange, Injection
 
Descriptive Properties
AdditivesRelease agent
Drying RecommendedyesInjection
FMVSS ClassBISO 3795 (FMVSS 302)
Fogging (mg)0G-value (condensate); ISO 6452; DAM
ISO designationISO 16396-PA6,GF15,M1GNR,S14-060
Max. screw tangential speed (m/s)0.2Injection
Odor Class4VDA 270; DS
Part Marking Code>PA6-GF15<ISO 11469
PolymerPA6-GF15
Processing Hold Pressure Time (s/mm)3Injection
Resin IdentificationPA6-GF15ISO 1043

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Celanese Zytel® 73G15HSL BK363 PA6-GF15
Ravago Manufacturing Americas Hylon® N1000EHL Nylon 6/6 (DAM)
RTP Company RTP 200 UV  Nylon 6/6 (PA 6/6) UV Stable
Celanese Zytel® HTN51G15HSL NC010 PA6T/XT-GF15
Ravago Manufacturing Americas Hylon N1000EHL Nylon 66

PDSX5351 / 197991

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.