MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
AGC Fluon® P-805UP PFA Perfluoropolymer
Categories: Polymer; Thermoplastic; Fluoropolymer; Perfluoroalkoxy (PFA); Polyperfluoroalkoxyethylene, Molded/Extruded

Material Notes: Fluon® PFA is a copolymer of tetrafluoroethylene (C2F4) and perfluoroalkoxyethylene, which has excellent chemical, electrical, mechanical and surface properties. PFA retains many inherent characteristics and similar properties of PTFE but can be processed using conventional thermoplastic techniques, such as extrusion molding, injection molding, blow molding, or electrostatic powder coating. And Fluon® PFA can be used in a wide range of temperatures from extremely low to high temperatures (260°C at the maximum) without losing its superior properties.

Information provided by Asahi Glass Company, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 2.12 - 2.17 g/ccASTM D792
Water Absorption <= 0.030 %ASTM D570
Melt Flow 3.0 - 7.0 g/10 min
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 60ASTM D1706
Tensile Strength at Break 36.0 MPaASTM D638
Tensile Strength, Ultimate 12.0 MPa
@Temperature 250 °C
ASTM D638
Elongation at Break 390 %ASTM D638
 680 %
@Temperature 250 °C
ASTM D638
Flexural Modulus 0.590 GPaASTM D790
Izod Impact, Notched NBASTM D256A
Coefficient of Friction, Dynamic 0.20
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+18 ohm-cmASTM D257
Surface Resistance >= 1.00e+17 ohmASTM D257
Dielectric Constant <= 2.1
@Frequency 60 Hz
ASTM D150
 <= 2.1
@Frequency 1000 Hz
ASTM D150
 <= 2.1
@Frequency 1e+6 Hz
ASTM D150
Dissipation Factor <= 0.00020
@Frequency 60 Hz
ASTM D150
 <= 0.00020
@Frequency 1000 Hz
ASTM D150
 <= 0.00020
@Frequency 1e+6 Hz
ASTM D150
Arc Resistance >= 300 secASTM D495
 
Thermal PropertiesOriginal ValueComments
CTE, linear 130 µm/m-°C
@Temperature 20.0 °C
ASTM D696
Specific Heat Capacity 1.046 J/g-°C
Thermal Conductivity 0.251 W/m-KASTM C177
Melting Point 305 - 315 °C
Maximum Service Temperature, Air 260 °CContinuous
Flammability, UL94 V-0
Oxygen Index >= 95 %ASTM D2863
 
Descriptive Properties
Ball Pressure Temperature, °C230
Flex Life, Cycles200000

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Daikin NEOFLON® AF-0012 PFA Film
Daikin NEOFLON® AF-1150 PFA Film
Daikin NEOFLON® AP-201 PFA
AGC Fluon® P-66P PFA Resin
Honeywell ACLAR® CX 130E Heat Sealable PCTFE Film

PAGC81 / 23040

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.