MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
SABIC PP 49MK40 Polypropylene Impact Copolymer for Injection Molding  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Impact Modified; Molded/Extruded

Material Notes: Product Description: PP 49MK40 is a high crystalline impact copolymer with high stiffness. This grade is especially developed for producing injection molded articles. The grade contains an antistatic & nucleating agent and has medium flow properties, medium impact resistance (even at low temperature) and high stiffness.

Typical Applications: PP 49MK40 can be used for general purpose IM products that require high stiffness, such as housewares, garden furniture, appliances and rigid packaging.

Information provided by SABIC.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.905 g/ccASTM D792
Linear Mold Shrinkage 0.012 - 0.025 cm/cm
Melt Flow 18 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 88ASTM D785
Tensile Strength, Yield 33.0 MPaASTM D638
Elongation at Yield 5.0 %ASTM D638
Flexural Modulus, 1% Secant 1750 MPaASTM D790A
Izod Impact, Notched 38.0 J/m
@Temperature -20.0 °C
ASTM D256
 60.0 J/m
@Temperature 23.0 °C
ASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 100 °CASTM D648
Vicat Softening Point 155 °CASTM D1525B
 
Processing PropertiesOriginal ValueComments
Processing Temperature 200 - 240 °CBarrel Temperature
Mold Temperature 15.0 - 40.0 °C

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LyondellBasell Pro-fax 8523 Polypropylene Impact Copolymer
Chevron Phillips Marlex® AHN-230 Polypropylene Impact Copolymer
Chevron Phillips Marlex® AHM-200 Polypropylene Impact Copolymer
Chevron Phillips Marlex® AHX-006 Polypropylene Impact Copolymer
LyondellBasell Montell SE191 Polypropylene Impact Copolymer

PSABICZ870 / 133066

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.