MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Persian Gulf Polymer HDPE-HFI 5110 Film Grade
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Film Grade

Material Notes: HFI5110 is a high molecular weight, high density polyethylene, which has a broad molecular weight distribution and high melt strength. This product specially designed for producing thin films with excellent strength and rigidity. Typical Applications: HFI5110 is recommended for blown film extrusion. This product is suitable for manufacture of high strength grocery sacks, shopping bags and high quality thin films for uni/multi-wall packaging. Films produced with this product can be readily treated and printed to give high quality graphics.

Information provided by Persian Gulf Polymer - Pooya Tejarat Novin Co.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.951 g/cc0.0344 lb/in³ISO 1183
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 26.0 MPa3770 psiISO 527-1
Film Elongation at Break, MD 580 %580 %ISO 527-1
Film Elongation at Break, TD 620 %620 %ISO 527-1
Elongation at Yield 10 %10 %ISO 527-1
Modulus of Elasticity 1.05 GPa152 ksiISO527-1;2
 
Thermal PropertiesMetricEnglishComments
Melting Point 132 °C270 °FISO 3146
Vicat Softening Point 127 °C
@Load 1.02 kg
261 °F
@Load 2.25 lb
A50, 50°C/h; ISO 306

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PPERSI939 / 250343

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.