MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LATI Latiblend 5262 PP Homopolymer/PA6
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Unreinforced; Polypropylene (PP)

Material Notes: Blend based on Polypropylene homopolymer (PPh) / Polyamide 6 (PA6). Unfilled. High impact resistance. Very good elongation.

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Information provided by Lati Industria Termoplastici S.p.A.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.970 g/cc0.0350 lb/in³
Linear Mold Shrinkage, Flow 0.013 - 0.017 cm/cm0.013 - 0.017 in/in
Linear Mold Shrinkage, Transverse 0.014 - 0.018 cm/cm0.014 - 0.018 in/in
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 20.0 MPa2900 psi
Elongation at Break 150 %
@Temperature 23.0 °C
150 %
@Temperature 73.4 °F
Elongation at Yield 6.0 %
@Temperature 23.0 °C
6.0 %
@Temperature 73.4 °F
Tensile Modulus 0.750 GPa109 ksi
Charpy Impact Unnotched NBNB
Charpy Impact, Notched 3.00 J/cm²14.3 ft-lb/in²
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 70.0 °C158 °F
Deflection Temperature at 0.46 MPa (66 psi) 80.0 °C176 °F
Deflection Temperature at 1.8 MPa (264 psi) 45.0 °C113 °F
Vicat Softening Point 70.0 °C
@Load 5.00 kg
158 °F
@Load 11.0 lb
 
Processing PropertiesMetricEnglishComments
Melt Temperature 220 - 240 °C428 - 464 °F
Mold Temperature 70.0 - 80.0 °C158 - 176 °F
Drying Temperature 80.0 - 90.0 °C
@Time 10800 sec
176 - 194 °F
@Time 3.00 hour
 
Descriptive Properties
ISO Shrinkage - Pressure60 MPa

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LATI Latiblend 6252 H2 G/30 PA6/PP Homopolymer
Ineos K44-24-122 HDPE

PLATH9789 / 177485

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.