MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Epoxy Technology EPO-TEK® OG178 UV Cure Optical Epoxy
Categories: Polymer; Thermoset; Epoxy

Material Notes: Material Description: A single component, UV/visible shifted light curable epoxy, designed for adhesive, sealing, coating and encapsulating applications found in semiconductor, electro-optics, fiber optics, medical, and scientific/OEM industries. It is a low viscosity, all-purpose adhesive.

Information Provided by Epoxy Technology

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.15 g/cc
Viscosity 300 - 600 cP
@Temperature 23.0 °C
100 rpm
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 86
Tensile Modulus 221000 psiStorage
Shear Strength >= 3400 psiDie
 
Thermal PropertiesOriginal ValueComments
CTE, linear 68.0 µm/m-°CBelow Tg
 185 µm/m-°CAbove Tg
Maximum Service Temperature, Air 125 °CContinuous
 225 °CIntermittent
Minimum Service Temperature, Air -55.0 °CContinuous
 -55.0 °CIntermittent
Glass Transition Temp, Tg >= 50.0 °CPost-Cure Dynamic Scan 20200°C; Ramp -40200°C @ 20°C/Min
Decomposition Temperature 296 °CDegradation Temperature
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.528
@Wavelength 589 nm
Transmission, Visible >= 95 %
@Wavelength 380 - 520 nm
Spectral
 >= 99 %
@Wavelength 541 - 1660 nm
Spectral
 
Processing PropertiesOriginal ValueComments
Shelf Life 12.0 Monthrefrigerated
 
Descriptive Properties
ColorClear Orangebefore cure
ConsistencyPourable liquid
Number of ComponentsSingle
Weight Loss2.45%200°C
 3.19%250°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Master Bond UV10TKMed One component UV curable, biocompatible, high viscosity compound
MarkeTech Yttrium Vanadate (YVO4) Fiber Optic Crystal
MarkeTech Rutile (TiO2) Fiber Optic Crystal
Epoxy Technology EPO-TEK® OG142 UV Cure Optical Epoxy
Epoxy Technology EPO-TEK® H54 High Temperature Epoxy

PPOXYT169 / 141208

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.