MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Ovation Polymers SOFTAPLAS™ R 60300 GF Nat Thermoplastic Polyurethane, 30% Glass Fiber
Categories: Polymer; Thermoplastic; Polyurethane, TP; Thermoplastic Polyurethane (TPUR), Glass Fiber Reinforced

Material Notes: 30% short glass fiber reinforced for excellent strength and processability

All properties after 48hrs conditioning at 23°C/50% RH

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.45 g/cc1.45 g/ccASTM D792
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 80.0 MPa11600 psi50 mm/min; ASTM D638
Elongation at Break 13 %13 %50 mm/min; ASTM D638
Tensile Modulus 2.45 GPa355 ksi50 mm/min; ASTM D638
Flexural Strength 90.0 MPa13100 psi1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 2.75 GPa399 ksi1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 2.94 J/cm
@Temperature 23.0 °C
5.50 ft-lb/in
@Temperature 73.4 °F
ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 78.0 °C
@Thickness 3.20 mm
172 °F
@Thickness 0.126 in
Unannealed; ASTM D648

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Ovation Polymers Nima™ NH PC143P Polycarbonate
Ovation Polymers Nemcon™ H PO DP 117/X2 Polyolefin, Thermally conductive
Ovation Polymers Nemcon™ H PC DP120/X3 BK Polycarbonate, Thermally Conductive, Black
Ovation Polymers Nemcon™ H PC DP120/X2 Polycarbonate, Thermally Conductive
Ovation Polymers Nemcon™ H PA DP117/X3 Polyphthalamide, Thermally Conductive

POVAT156 / 79135

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.