MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Copper Alloy, UNS C89545, M01 Temper, As Sand Cast
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Temper: As Sand Cast

Casting Characteristics: High – Shrinkage in Solidification; Medium – Casting Yield, Drossing, Effect of Section Size, Fluidity, Gassing

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.25 g/cc0.298 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell >= 70
@Load 500 kg
>= 70
@Load 1100 lb
Tensile Strength >= 214 MPa>= 31000 psi
 255 MPa37000 psiTypical
Tensile Strength, Yield >= 68.9 MPa>= 10000 psi0.2% Offset
 96.5 MPa14000 psi0.2% Offset, Typical
Elongation at Break >= 2.0 %>= 2.0 %
Tensile Modulus 93.1 GPa13500 ksi
Modulus of Rigidity 35.2 GPa5100 ksi
Poissons Ratio 0.320.32
Izod Impact >= 40.7 J>= 30.0 ft-lb
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000800 ohm-cm0.00000800 ohm-cm21.4% IACS
 
Thermal PropertiesMetricEnglishComments
CTE, linear 18.7 µm/m-°C
@Temperature 20.0 - 300 °C
10.4 µin/in-°F
@Temperature 68.0 - 572 °F
Thermal Conductivity 8.17 W/m-K56.7 BTU-in/hr-ft²-°F
Melting Point 878.9 - 922.2 °C1614 - 1692 °F
Solidus 878.9 °C1614 °F
Liquidus 922.2 °C1692 °F
Shrinkage 1.56 %1.56 %Patternmaker's Shrinkage (3/16 in./ft.)
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 0.60 - 1.5 %0.60 - 1.5 %
Bismuth, Bi 0.20 - 0.90 %0.20 - 0.90 %
Boron, B <= 0.020 %<= 0.020 %
Copper, Cu 66 - 72 %66 - 72 %
Iron, Fe <= 0.30 %<= 0.30 %
Lead, Pb <= 0.090 %<= 0.090 %
Manganese, Mn <= 0.30 %<= 0.30 %
Phosphorus, P 0.010 - 0.15 %0.010 - 0.15 %
Silicon, Si <= 0.30 %<= 0.30 %
Tin, Sn <= 0.50 %<= 0.50 %
Zinc, Zn 27 - 31 %27 - 31 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

MC89545x1 / 292582

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.