Notes: 66GS6 is a 30% glass sphere filled nylon 66 that offers increased rigidity coupled with low distortion Features: High Rigidity; Low Warpage Processing Method: Injection Molding Forms: Pellets Injection Notes: No drying is necessary unless the material has been exposed to air for longer than 3 hours; Back Pressure: Low; Injection Pressure: High; Injection Rate: Fast Information Provided by Teknor Apex |