MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Hexcel® ML-10019 ML-79 Series urethane foam
Categories: Other Engineering Material

Material Notes: Description:
  • Broadband, multilayer absorber consisting of graduated layers of loaded open-cell urethane foam.
  • Ideal for antenna cross-talk, side lobe reduction, cavity resonance suppression, and far-field electromagnetic applications.
  • Available with PSA, conductive film backing, and acrylic surface coating - When ordered in sheet form, ARC P/N will be indicated on the back-side or mounting surface.
  • Can be water-jet cut for custom configurations.
  • RoHS and REACH compliant.

Information provided by Hexcel Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Thickness 114000 microns4500 milStandard
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 132 °C270 °F
Minimum Service Temperature, Air -57.0 °C-70.6 °F
 
Descriptive Properties
ColorBlack
Reflection Loss=-17 dB
Reflectivity Range2 - 18 GHz

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PHEXCB9337 / 322493

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.