MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Dover Chemical DOVERGUARD 245 Flame Retardant Additive
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Doverguard 245, a brominated cyanurate, is a proprietary, additive flame retardant. The combination of aromatic bromine and cyanurate provides high FR efficiency and good thermal stability. A major use of Doverguard 245 is in ABS and HIPS. Doverguard 245 combines good UV, impact and flow properties. It is non-blooming.

Information provided by DoverChem

Key Words: CAS# 25713-60-4
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 2.44 g/cc
Volatiles 0.10 %
Solubility in Water 0.00 %
Solubility 2000 ppm
@Temperature 25.0 °C
Methanol
 30000 ppm
@Temperature 25.0 °C
Methylene Acetate
 40000 ppm
@Temperature 25.0 °C
Methyl Ethyl Ketone
 170000 ppm
@Temperature 25.0 °C
Carbon Tetrachloride
 280000 ppm
@Temperature 25.0 °C
Toluene
 
Thermal PropertiesOriginal ValueComments
Melting Point 230 °C
 
Descriptive Properties
AppearanceWhite Powder
Assay, %99.8HPLC
Bromine, %67
Loss on Drying, %1010mg @ 10°C/minute, air; @ 400°C
 210mg @ 10°C/minute, air; @ 360°C
 510mg @ 10°C/minute, air; @ 365°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

WDOVER016 / 217635

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.