MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

(Viewing data as-entered. Click here to return)
Syensqo (Solvay Specialty Polymers) Torlon® 4275 PAI, Good wear resistance at high velocities
Categories: Polymer; Thermoplastic; Polyamide-imide (PAI); Polyamide-Imide, Graphite Filled

Material Notes: Good wear resistance at high velocities, contains PTFE and graphite

Torlon® 4275 is a wear-resistant grade of polyamide-imide (PAI). This grade offers an excellent balance of mechanical properties and wear resistance. It offers high tensile strength and modulus with a low coefficient of friction and outstanding wear resistance at both high velocity and high pressure conditions.

Torlon® PAI has the highest strength and stiffness of any thermoplastic up to 275°C (525°F). It has outstanding resistance to wear, creep and chemicals.

Potential applications for Torlon® 4275 polyamide-imide include thrust washers, spline liners, valve seats, bushings, bearings, wear rings, cams and other applications requiring strength at high temperature and resistance to wear.

Applications: Aerospace Applications; Aircraft Applications; Automotive Applications; Bearings; Bushings; Gears; Industrial Applications; Industrial Parts; Machine/Mechanical Parts; Metal Replacement; Rollers; Sealing Devices; Seals; Thrust Washer; Transmission Applications; Washer

Features: Chemical Resistant; Creep Resistant; Flame Retardant; High Heat Resistance; High Temperature Strength; Low Friction; Self Lubricating; Semi Conductive; Wear Resistant

Injection notes: Minimum drying conditions: 3 hours at 350°F (177°C), 4 hours at 300°F (149°C), or 16 hours at 250°F (121°C).
Compression Ratio: 1:1 to 1.5:1
Begin hold pressure at a high setting 6,000-8,000 psi (41.37-55.16 MPa), for several seconds, then drop off to 3,000-5,000 psi (20.69-34.48 MPa), for the duration of the hold pressure sequence.
Molded parts must be post cured.

Information provided by Solvay Specialty Polymers.

Vendors: Drake extrudes shapes and machines and injection molds parts in Torlon® PAI, PEEK, PAEK, Ryton PPS and Ultem PEI. It also machines Vespel® PI. Innovations include cryogenic CryoDyn® CT-200 shapes as a PCTFE alternative; efficient Seamless Tube® and the largest extruded rod diameters to >254mm and plate thicknesses to > 100mm. Certified to ISO 9001:2015 and AS9100D. Visit www.DrakePlastics.com

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.51 g/ccASTM D792
Water Absorption 0.33 %
@Time 86400 sec
ASTM D570
Linear Mold Shrinkage, Flow 0.0025 - 0.0045 cm/cmASTM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 117 MPaASTM D638
Tensile Stress 131 MPaASTM D1708
Tensile Modulus 7790 MPaASTM D638
 8830 MPaASTM D638
Flexural Strength 110 MPa
@Temperature 232 °C
ASTM D790
 208 MPa
@Temperature 23.0 °C
ASTM D790
Flexural Modulus 5100 MPa
@Temperature 232 °C
ASTM D790
 7310 MPa
@Temperature 23.0 °C
ASTM D790
Compressive Strength 123 MPaASTM D695
Compressive Modulus 4000 MPaASTM D695
Izod Impact, Notched 85.0 J/mASTM D256
Izod Impact, Unnotched 270 J/mASTM D256
Coefficient of Friction 0.050 - 0.31ASTM D1894
K (wear) Factor 1.40 x 10-8 mm³/N-M
@Pressure 5.20 MPa
0.38 m/sec; ASTM D3702
 26.0 x 10-8 mm³/N-M
@Pressure 3.40 MPa
0.25 m/sec; ASTM D3702
 26.0 x 10-8 mm³/N-M
@Pressure 3.40 MPa
0.25 m/sec; ASTM D3702
 35.0 x 10-8 mm³/N-M
@Pressure 0.220 MPa
4.1 m/sec; ASTM D3702
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 8.00e+15 ohm-cmASTM D257
Surface Resistance 4.00e+17 ohmASTM D257
 
Thermal PropertiesOriginal ValueComments
CTE, linear 25.0 µm/m-°CASTM D696
Thermal Conductivity 0.650 W/m-KASTM C177
Deflection Temperature at 1.8 MPa (264 psi) 280 °CUnannealed; ASTM D648
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 304 °C
Nozzle Temperature 371 °C
Mold Temperature 199 - 216 °C
Drying Temperature 177 °C
@Time 10800 sec
Moisture Content <= 0.050 %Injection
Back Pressure 6.89 MPa
Screw Speed 50 - 100 rpm
 
Descriptive Properties
AdditivePTFE + Graphite Lubricant
AvailabilityAsia Pacific
 Europe
 Latin America
 North America
FormsPellets
ProcessingInjection Molding; Machining; Profile Extrusion
RoHS ComplianceYes
Screw L/D Ratio, Injection18.0:1.0 to 24.0:1.0

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSOL8Y4546 / 280346

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.