Description: Conoco Hydroclear Spindle Oil is a high-quality needle- and spindlebearing lubricant formulated from premium Conoco hydrocracked base stocks. Hydroclear Spindle Oil is specially formulated with proprietary additive chemistry and oiliness agents, and is recommended for use in the lubrication of high-speed needle and spindle bearings typically found in agriculture and textile equipment. Hydroclear Spindle Oil is also ideally suited for use in machine tools and other equipment where a low-viscosity, thermally stable lubricant is required. Hydroclear Spindle Oil is available in an ISO 15 viscosity grade. Information provided by ConocoPhillips. Phillips 66 Lubricants was spun-off from ConocoPhillips in 2012, and branding was further reorganized in 2016. The Hydroclear® trade name is no longer in use but products may be available under different names. |