Hostacom EP3307 T 8051 is an unfilled polypropylene copolymer, with high impact resistance and good UV resistance. Product is available as a customized color matched, pellet form. This grade is delivered in 8051 color version. This product is also available in other colors, new colors can be developed depending on customer requirements. Applications: Interior TrimsInformation provided by LyondellBasell. |