LNP STAT-LOY A3000TXB compound is based on Acrylonitrile Butadiene Styrene (ABS) resin containing proprietary fillers. Added features of this grade include: Permanently Anti-Static, Transparent, Bio-assessed to ISO 10993. Features: Biocompatible,Antistatic,Transparent Information provided by SABIC |