MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Domo TECHNYL® 2417IG PA66, 20% glass fiber, DRY
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 20% Glass Fiber Filled

Material Notes: Description: Polyamide 66, 20% glass fiber reinforced, Impact modified for injection molding.

Available in: Asia Pacific

Product Applications: TECHNYL® 2417IG4 is used in all sectors of industries, offering good mechanical strength, impact strength for injection molding. This grade is widely used for: Distributor pipe. This product is available in natural color and in colors on request.

DOMO Chemicals has acquired Solvay’s Performance Polyamides Business in Europe.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.23 g/ccASTM D792
Linear Mold Shrinkage, Flow 0.0070 - 0.010 cm/cm
Linear Mold Shrinkage, Transverse 0.0070 - 0.010 cm/cm
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 140 MPaASTM D638
Elongation at Break 4.0 %ASTM D638
Flexural Strength 200 MPaASTM D790
Flexural Modulus 7500 MPaASTM D790
Izod Impact, Notched 180 J/mASTM D265
 
Thermal PropertiesOriginal ValueComments
Melting Point 262 °CISO 11357
Deflection Temperature at 1.8 MPa (264 psi) 250 °CASTM D648
Flammability, UL94 HB
@Thickness 3.20 mm
ISO 1210
 
Processing PropertiesOriginal ValueComments
Feed Temperature 270 - 280 °C
Mold Temperature 70.0 - 100 °C
Drying Temperature 80.0 °C
Moisture Content <= 0.20 %
 
Descriptive Properties
Compression Zone275-285°C
Mixing Zone280-290°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Plastcom SLOVAMID 66 GF 20 PA66, 20% glass fibre
Domo TECHNYL® A 216 V20 PA66, 20% glass fiber, DRY
Envalior Durethan® ECO BKV 20 FN20 000000 Nylon 6 (PA6), 20% Glass Fiber Reinforced, Conditioned
Domo TECHNYL® A 218 V20 Black 21N PA66, 20% glass fiber, Conditioned
Plastcom SLOVAMID 66 GF 20 GF 10 PA66, 20% glass fibre, glass beads

PRHOD577 / 137808

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.