MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Covestro Makrolon® FR 7067 Polycarbonate  (discontinued **)
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Molded; Polycarbonate, Unreinforced, Flame Retardant; Polycarbonate, UV Stabilized

Material Notes: Main characteristics:
• High toughness
• Good heat resistance
• Glass-like transparency, optical quality
• High dimensional accuracy and stability

Grade characteristics:
• Flame retardant
• Medium viscosity, easy release
• UV stabilized

As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Melt Flow 20 g/10 min
@Load 1.20 kg,
Temperature 300 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 75.0 MPa50 mm/min; ISO 527-1,-2
Tensile Strength, Yield 75.0 MPa50 mm/min; ISO 527-1,-2
Elongation at Break 100 %50 mm/min; b.o. ISO 527-1,-2
Elongation at Yield 5.0 %50 mm/min; ISO 527-1,-2
Tensile Modulus 2600 MPa1 mm/min; ISO 527-1,-2
Charpy Impact Unnotched NB
@Temperature 23.0 °C
ISO 179-1eU
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 105 °CISO 75-1,-2
Deflection Temperature at 1.8 MPa (264 psi) 95.0 °CISO 75-1,-2
Vicat Softening Point 123 °C
@Load 5.10 kg
50°C/h; ISO 306
UL RTI, Electrical 80.0 °CUL 746B
UL RTI, Mechanical with Impact 80.0 °CUL 746B
UL RTI, Mechanical without Impact 80.0 °CUL 746B
Flammability, UL94 V-0
@Thickness 1.50 mm
 V-0
@Thickness 3.00 mm
 5VA
@Thickness 3.00 mm
UL-94 5V
Glow Wire Ignition Temperature 960 °C
@Thickness 1.50 mm
IEC 60695-2-13
 960 °C
@Thickness 3.00 mm
IEC 60695-2-13
Glow Wire Flammability Index 960 °C
@Thickness 1.50 mm
IEC 60695-2-12
 960 °C
@Thickness 3.00 mm
IEC 60695-2-12
 
Optical PropertiesOriginal ValueComments
Haze 2.0 %
@Thickness 3.00 mm
ISO 14782
Transmission, Visible 88 %
@Thickness 3.00 mm
ISO 13468-2
 
Processing PropertiesOriginal ValueComments
Melt Temperature 280 °CInjection molding; ISO 294
Mold Temperature 80.0 °CInjection molding; ISO 294
Injection Velocity 200 mm/secISO 294

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Covestro Makrolon® FR 7087 Polycarbonate
Covestro Makrolon® 6255 Polycarbonate
Covestro Makrolon® 2800 Polycarbonate
Covestro Makrolon® 6165 X Polycarbonate
Covestro Makrolon® 6485 Polycarbonate, Injection Grade

PB09641 / 150773

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.