MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Dow Dow™ DFDA-7074 NT7 LLDPE
Categories: Polymer; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Film Grade

Material Notes: Product Description: Dow DFDA-7074 NT7 linear low density polyethylene is an ethylene-butene copolymer designed for blown film applications.
Main Characteristics:
  • Butene linear low density polyethylene
  • Blown film extrusion
  • Pellet form
Complies with: US FDA 21 CFR 177.1520©3.2a; Canadian HPFB No Objection (with Limitations); EU No 10/2011; JHOSPA. Consult the regulations for complete details.

Availability: Europe; North America

Additive: Antiblock: No; Processing Aid: No; Slip: No

Agency Ratings: FDA 21 CFR 177.1520©3.2a; Canadian HPFB No Objection; EU No 10/2011; JHOSPA

Form: Pellets

Processing Method: Blown Film

Information provided by The Dow Chemical Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.920 g/cc0.0332 lb/in³ASTM D792
Melt Flow 1.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
1.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Puncture Resistance 35.6 N8.00 lb (f)
Film Tensile Strength at Yield, MD 10.7 MPa1550 psiASTM D882
Film Tensile Strength at Yield, TD 11.0 MPa1600 psiASTM D882
Film Elongation at Break, MD 580 %580 %ASTM D882
Film Elongation at Break, TD 690 %690 %ASTM D882
1% Secant Modulus 221 MPa32000 psiMD; ASTM D882
 248 MPa36000 psiTD; ASTM D882
2% Secant Modulus 0.189 GPa27.4 ksiMD; ASTM D882
 0.210 GPa30.4 ksiTD; ASTM D882
Puncture Energy 2.49 J1.83 ft-lb
Elmendorf Tear Strength MD 170 g170 gMethod B; ASTM D1922
Elmendorf Tear Strength TD 320 g320 gMethod B; ASTM D1922
Dart Drop Test 90.0 g0.198 lbASTM D1709A
Film Tensile Strength at Break, MD 36.5 MPa5300 psiASTM D882
Film Tensile Strength at Break, TD 26.9 MPa3900 psiASTM D882
 
Thermal PropertiesMetricEnglishComments
Melting Point 121 °C250 °F
Vicat Softening Point 102 °C216 °FASTM D1525
 
Optical PropertiesMetricEnglishComments
Haze 19 %19 %ASTM D1003
Gloss 33 %33 %45°; ASTM D2457
 
Processing PropertiesMetricEnglishComments
Melt Temperature 216 °C420 °FExtrusion
Blow-up Ratio (BUR) 2.52.5
 
Descriptive Properties
Film Puncture Resistance145 ft-lb/in3
Film Toughness1150 ft-lb/in3TD, ASTM D882
 1170 ft-lb/in3MD, ASTM D882

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PDOWF477 / 311170

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.