Telcar TL-1445S is a general purpose thermoplastic elastomer designed for industrial market. This product is a stable and is designed for extrusion processes. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America Features: Filled; Light Stabilized; Low Flow; Medium Density; Medium Hardness; Slip; Sunlight Resistant Uses: General Purpose; Weatherstripping RoHS Compliant:RoHS Form: Pellets Processing Method: Extrusion Information provided by Teknor Apex |