MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

(Viewing data as-entered. Click here to return)
CoorsTek Epoxy Seal 923 (ES-923) B-staged epoxy lids
Categories: Polymer; Thermoset; Epoxy

Material Notes: ES-923 is designed for applications requiring a rapid epoxy cure cycle (10 minutes at 160° C). This accelerated seal cycle results in only a modest reduction in moisture resistance and seal strength from the ES-216 epoxy.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 90
Shear Strength 2600 psiLap Shear; ASTM D1002
 
Thermal PropertiesOriginal ValueComments
CTE, linear 50.0 µm/m-°CMIL STD 883D
Thermal Conductivity 0.500 W/m-KMIL STD 883D
Maximum Service Temperature, Air 180 °CContinuous
 220 °CIntermittent
 
Processing PropertiesOriginal ValueComments
Cure Time 0.1667 hour
@Temperature 160 °C
 
Descriptive Properties
ColorYellow
Gross LeakPass
Moisture ResistancePass, 144 hrs. @ 121° C & 100% RH
 Pass, 200 hrs. @ 85° C & 85% RH
Temperature CyclingPassMIL STD 883D
Thermal Shock Resistance (°C)PassMIL STD 883D

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Epoxy Technology EPO-TEK® H67-MP Thermally Conductive Epoxy
Park Aerospace Nelco® N4000-29 BC® Buried Capacitance™ Multifunctional Epoxy
Epoxy Technology EPO-TEK® T7139 Glob Top Epoxy
Epoxy Technology EPO-TEK® T6067 Thermally Conductive, Electrically Insulating Epoxy
Epoxy Technology EPO-TEK® H70E-4 Thermally Conductive Epoxy

PCOOR919 / 104623

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.