MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Hexcel® Redux® 308 Modified epoxy film adhesive
Categories: Polymer; Adhesive; Film; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: Redux 308 is a high-strength film adhesive curing at 350°F. It is suitable for a wide range of structural bonding applications including metal to metal bonding and sandwich constructions, where operating temperatures of up to 250°F may be experienced.

Features: Cures at 350°F; Good structural performance and service temperature up to 250°F; Excellent environmental resistance; Superior aging performance for continuous operation up to 250°F; Low volatile content (solventless process).
Applications: Metal to metal bonding; Structural sandwich constructions

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 1.16 ksi
@Temperature 21.1 °C
Flatwise Tensile
Shear Strength 2.90 ksi
@Temperature 121 °C
Lap Shear
 6.30 ksi
@Temperature 71.1 °C
Lap Shear
 6.80 ksi
@Temperature 21.1 °C
Lap Shear
Peel Strength 27.0 pli
@Temperature 21.1 °C
Bell Peel
 
Processing PropertiesOriginal ValueComments
Shelf Life 12.0 Month
@Temperature -17.8 °C
 
Descriptive Properties
Areal Weight (psf)0.06
Roll Width (in)39
Standard Roll (ft2)540

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Master Bond EP46HT-1 Epoxy For High Temperature Service
Master Bond EP45HTQ Quartz Filled Heat Resistant Epoxy
Epoxy Technology EPO-TEK® 353ND-T High Temperature Thixotropic Epoxy
Abatron AboCast 50-3/AboCure 8110-1 Flexible Epoxy
ArcelorMittal FB 450 Hot rolled ferrite-bainite steel

PHEXC432 / 99251

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.