Introduction: It is a two component room temperature vulcanizing pour able fluid silicon which cures on the addition of the appropriate CATALYST S o SN, according to the polycondensation process. SILIMOLD AL-10 silicon rubber is characterized by its low hardness and a high tearing resistance. Thanks to these properties, it may also be utilized in the manufacture of moulds with many undercuts. Application: SILIMOLD AL-10 silicon rubber is ideal in the manufacture of moulds for the production of articles made from synthetic resins (polyester, epoxy polyurethane, etc), plaster, cement, wax etc. It is also suitable for the" wasted wax "process in the artistic casting and founding. Note 1: Tests have been carried out under these conditions: Temperature: +20°C; After: 24 ore; R.H.: 60%; Catalysis: 100:5 Information provided by Poolkemie |