MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Evonik DYNAPOL® S 1606 Linear Copolyester
Categories: Polymer; Thermoplastic; Polyester, TP

Material Notes: A saturated, linear copolyester, amorphous. Generally used in a solution, film or melt from heated tanks or extruders for the adhesion of metals, PVC, polyester foil and PE-foam.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.30 g/ccDIN 53 479
Viscosity 90000 cP
@Temperature 220 °C
melt; (Plate/Plate)
 150000 cP
@Temperature 200 °C
melt; (Plate/Plate)
Viscosity Test 58 - 66 cm³/gDIN 53 728
Melt Flow 30 g/10 min
@Temperature 200 °C
DIN ISO 1133
 30 g/10 min
@Temperature 220 °C
DIN ISO 1133
 
Chemical PropertiesOriginal ValueComments
Total Acid Number <= 3.0DIN EN ISO 2114
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 80
Tensile Strength, Ultimate 40.0 MPaDIN EN ISO 527-1/3
Elongation at Break 3.0 %
 
Thermal PropertiesOriginal ValueComments
Softening Point 150 °CDIN ISO 4625
Glass Transition Temp, Tg 65.0 °CDIN 53 765
 
Descriptive Properties
Hydroxyl Number (mg KOH/g)>2DIN 53 240-2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
EMS-Griltech Griltex® 6E Copolyester Hotmelt Adhesive (Apparel Interlinings)
Envalior Arnitel® PL381 Injection Molding Grade Copolyester Elastomer (North America)
Evonik DYNAPOL® LH 830 Polyester Resin
EMS-Griltech Griltex® D 1519E Copolyester Hotmelt Adhesive (Technical Applications)
EMS-Griltech Griltex® D 1441E Copolyester Hotmelt Adhesive (Technical Applications)

PHUMB270 / 81272

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.