MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Chemours Teflon® PTFE Grade 7B Granular Compression Molding Resin  (discontinued **)
Categories: Polymer; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE)

Material Notes: DuPont™ Teflon® PTFE 7B is a white granulated powder with an ultra fine particle size and high bulk density. The ultra-fine particle size minimizes voids even at relatively low molding pressure. Teflon® PTFE 7B is an excellent choice for moldings requiring optimum mechanical and electrical properties. The ultra-fine particle size of Teflon® PTFE 7B promotes good capture and uniform distribution of inorganic fillers when they are added to modify the mechanical properties of moldings. Teflon® PTFE 7B exhibits a mold shrinkage that is intermediate of the mold shrinkage of 7A and 7C grades.

Properly processed products made from neat Teflon® PTFE 7B provide the superior properties typical of the fluoropolymer resins: retention of properties after service at 260°C (500°F), useful properties at –240°C (–400°F), chemical inertness to nearly all industrial chemicals and solvents, and low friction and antistick surfaces. Dielectric properties are outstanding and stable with frequency and temperature. Molded products have moderate stiffness and high ultimate elongation. In a flame situation, products of Teflon® PTFE 7B resist ignition and do not themselves promote flame spread. When ignited by flame from other sources, their contribution of heat is small and with very little smoke.

Statements, or data, regarding behavior in a flame situation are not intended to reflect hazards presented by this or any other material when under actual fire conditions.

Applications

Many end products are molded or fabricated from moldings of Teflon® PTFE 7B—or made with filled compounds based on Teflon® PTFE 7B. The filled compounds provide a wide choice of modified mechanical properties. End products using Teflon® PTFE 7B include skived film and sheet, gaskets, bridge or pipeline bearing pads, piston rings, and diaphragms.

Chemours was formed from former DuPont performance chemicals businesses, including DuPont Fluoroproducts, in 2015.

Key Words: Polytetrafluoroethylene
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 2.16 g/ccASTM D4894
Bulk Density 0.330 g/ccASTM D4894
Water Absorption <= 0.010 %24 hours; ASTM D570
Particle Size 24 µmASTM D4894
Linear Mold Shrinkage 0.044 cm/cmat preform pressure of 35 Mpa; ASTM D4894
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 58ASTM D785
Hardness, Shore A 98ASTM D2240
Hardness, Shore D 50 - 65ASTM D2240
Tensile Strength, Ultimate 36.5 MPaASTM D4894
Elongation at Break 400 %ASTM D4894
Flexural Modulus 0.496 GPaASTM D790
Poissons Ratio 0.46approaches a limit of 0.50 at higher temperature
Izod Impact, Notched 189 J/mASTM D256
Coefficient of Friction 0.050 - 0.10ASTM D 1894
Coefficient of Friction, Dynamic 0.10V = 10 fpm; P= 800 - 1000 psi
 0.13V = 100 fpm; P= 80 - 100 psi
Coefficient of Friction, Static 0.050 - 0.080500 psi
K (wear) Factor 2500 x 10-10 in³-min/ft-lb-hrunlubricated vs. soft carbon steel
Limiting Pressure Velocity 1200 psi-ft/min
@Temperature 21.0 - 27.0 °C
at 10 fpm
 1800 psi-ft/min
@Temperature 21.0 - 27.0 °C
at 100 fpm
 2500 psi-ft/min
@Temperature 21.0 - 27.0 °C
at 1000 fpm
Taber Abrasion, mg/1000 Cycles 8.91000 cycles; CS-17F wheel
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+18 ohm-cmASTM D257
Surface Resistivity per Square >= 1.00e+18 ohmASTM D257
Dielectric Constant 2.1
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 18.0 kV/mm100 micrometers film; ASTM D149
Dissipation Factor <= 0.00010
@Frequency 1e+6 Hz
ASTM D150
Arc Resistance >= 300 secASTM D495
 
Thermal PropertiesOriginal ValueComments
CTE, linear 112 µm/m-°C
@Temperature -100 - 25.0 °C
 124 µm/m-°C
@Temperature 25.0 - 100 °C
 220 µm/m-°C
@Temperature 25.0 - 300 °C
 790 µm/m-°C
@Temperature 20.0 - 25.0 °C
Large volume change in the 18-25°C transition range
Specific Heat Capacity 1.20 J/g-°C
@Temperature 40.0 °C
 1.30 J/g-°C
@Temperature 150 °C
 1.40 J/g-°C
@Temperature 20.0 °C
 1.50 J/g-°C
@Temperature 260 °C
Thermal Conductivity 0.250 W/m-K
 0.300 W/m-K
@Temperature 20.0 - 260 °C
Melting Point 317 - 337 °CASTM D4894
Maximum Service Temperature, Air 260 °Cretains useful mechanical properties
Minimum Service Temperature, Air -268 °Cretains useful mechanical properties
 -79.0 °Cremains highly flexible
Flammability, UL94 V-0
Oxygen Index >= 95 %ASTM D2863
 
Processing PropertiesOriginal ValueComments
Processing Temperature 379 - 429 °CCure Temperature
 
Descriptive Properties
20% Hydrochloric Acid Transmission, g/100sq in.<0.01
50% Sodium Hydroxide Transmission, g/100sq in.<.01
Acetic Acid Transmission, g/100sq in.0.41
Acetone Transmission, g/100sq in.0.95
Acetophenone Transmission, g/100sq in.0.5
Benzene Transmission, g/100sq in.0.64
Carbon Tetrachloride Transmission, g/100sq in.0.31
Chemical/Solvent ResistanceExcellent
Detergent Resist. on grit-blasted aluminum, Hours624
Detergent Resistance on aluminum, Hours264
Detergent Resistance on grit-blasted steel, Hours24
Ethyl Acetate Transmission, g/100sq in.0.76
Folding Endurance, # cycles, .18-.20 mm>10^6
Heat of Combustion J/g5100ASTM D240
Hexane Transmission, g/100sq in.0.56
Piperidine Transmission, g/100sq in.0.04
Red Fuming Nitric Acid Transmission, g/100sq in.7.5-1.4
Salt Spray Resistance on aluminum, Hours>744
Salt Spray Resistance on steel, Hours192
Sulfuric Acid Transmission, g/100sq in.0.00001
Water Transmission, g/100sq in.0.4
Weather Resistance20Years unaffected in Florida Exposure

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Silicone Rubber
Ti30Nb ß titanium alloy
3M Dyneon™ PVDF 2066_0002 Fluoroplastic
Chemours Teflon® PTFE 7A Granular Molding Powder
Silicon, Si

PDU900A / 33298

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.