Celcon« LW90-F2 is an acetal copolymer formulated with a nominal 9 melt flow rate base polymer and a standard level of polytetrafluoroethylene filler (PTFE). It is designed for use in wear applications against plastic, metal, glass, or ceramic mating surfaces where silicone lubricants can not be tolerated.Information provided by Celanese |