MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Westlake Plastics

(Viewing data as-entered. Click here to return)
Westlake Plastics Propylux® CN-P Polypropylene (conductive)
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with Carbon Black Filler

Material Notes: Propylux® PP CN-P (Statically conductive polypropylene) is a carbon powder-filled polypropylene offering surface resistivity in the 10EE4 to 10EE6 ohm/sq range and broad chemical resistance. This material is a good choice when ESD protection is needed or to minimize static discharge in flammable environments.

Industry: Engineering; Semiconductor and ESD

Colors Available: Black

Attributes: Chemical Resistance

Shapes: Compression Sheet

Information provided by Westlake Plastics Co.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.960 g/ccASTM D792
Water Absorption 0.010 %
@Time 86400 sec
ASTM D570
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 21.0 MPaASTM D638
Elongation at Break 15 %ASTM D638
Flexural Strength 28.0 psiASTM D790
Flexural Modulus 965 MPaASTM D790
Izod Impact, Notched 3.50 ft-lb/inASTM D256
Izod Impact, Unnotched 17.5 ft-lb/inASTM D256
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 100 - 1.00e+6 ohm-cmASTM D257
Surface Resistance 100 - 1.00e+6 ohmASTM D257
Static Decay <= 0.10 secMil-B-81705-B
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 54.0 °CASTM D648
Flammability, UL94 HB
 
Descriptive Properties
ColorBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Polypropylene, Flame Retardant
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant
Kingfa FRABS V-0 Flame Retardant ABS

PWEST054 / 72734

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.