MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Overview of materials for High Density Polyethylene (HDPE), Injection Molded
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Injection Molded

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Injection Molded". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 0.924 - 0.995 g/ccAverage value: 0.954 g/cc Grade Count:522
Brightness 60.0 %Average value: 60.0 % Grade Count:10
Water Absorption 0.000 - 0.0700 %Average value: 0.0146 % Grade Count:13
Moisture Absorption at Equilibrium 0.0100 - 0.100 %Average value: 0.0360 % Grade Count:5
Particle Size 5.00 - 1200 µmAverage value: 614 µm Grade Count:4
Viscosity 32000 - 200000 cP
@Temperature 190 - 190 °C
Average value: 89000 cP Grade Count:7
 32000 - 200000 cP
@Shear Rate 300 - 5000 1/s
Average value: 89000 cP Grade Count:7
Viscosity Test 280 - 3800 cm³/gAverage value: 846 cm³/g Grade Count:7
Environmental Stress Crack Resistance 1.00 - 10000 hourAverage value: 379 hour Grade Count:142
 2.00 - 500 hour
@Temperature 50.0 - 80.0 °C
Average value: 115 hour Grade Count:33
 2.00 - 65.0 hour
@Temperature 50.0 - 50.0 °C
Average value: 115 hour Grade Count:13
 2.00 - 65.0 hour
@Thickness 0.300 - 2.00 mm
Average value: 115 hour Grade Count:13
Oxidative Induction Time (OIT) 20.0 - 100 minAverage value: 47.5 min Grade Count:4
 30.0 - 120 min
@Temperature 200 - 210 °C
Average value: 59.6 min Grade Count:14
Linear Mold Shrinkage 0.0100 - 0.0400 cm/cmAverage value: 0.0217 cm/cm Grade Count:32
Linear Mold Shrinkage, Transverse 0.00960 - 0.0300 cm/cmAverage value: 0.0201 cm/cm Grade Count:14
Melt Flow 0.0250 - 1610 g/10 minAverage value: 22.7 g/10 min Grade Count:514
Base Resin Melt Index 2.00 - 20.0 g/10 minAverage value: 7.00 g/10 min Grade Count:8
Spiral Flow 15.5 - 55.8 cmAverage value: 33.7 cm Grade Count:50
Ash 0.000 - 0.0500 %Average value: 0.0260 % Grade Count:5
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 33.0 - 66.0Average value: 48.7 Grade Count:7
Hardness, Shore D 50.0 - 76.0Average value: 64.5 Grade Count:270
Ball Indentation Hardness 40.0 - 58.0 MPaAverage value: 51.6 MPa Grade Count:17
Tensile Strength, Ultimate 7.60 - 43.0 MPaAverage value: 22.0 MPa Grade Count:207
Film Tensile Strength at Yield, MD 21.0 - 35.0 MPaAverage value: 28.9 MPa Grade Count:5
Film Tensile Strength at Yield, TD 23.0 - 37.5 MPaAverage value: 31.1 MPa Grade Count:5
Tensile Strength, Yield 11.0 - 43.0 MPaAverage value: 26.2 MPa Grade Count:448
Film Elongation at Break, MD 595 - 900 %Average value: 709 % Grade Count:5
Film Elongation at Break, TD 650 - 950 %Average value: 860 % Grade Count:5
Elongation at Break 3.20 - 2230 %Average value: 587 % Grade Count:352
Elongation at Yield 3.00 - 80.0 %Average value: 10.3 % Grade Count:130
Modulus of Elasticity 0.565 - 1.50 GPaAverage value: 0.995 GPa Grade Count:84
Flexural Yield Strength 13.8 - 48.3 MPaAverage value: 31.1 MPa Grade Count:14
Flexural Modulus 0.280 - 1.86 GPaAverage value: 1.14 GPa Grade Count:402
Secant Modulus 0.758 - 1.59 GPaAverage value: 1.03 GPa Grade Count:33
Izod Impact, Notched 0.0200 - 5340 J/cmAverage value: 0.809 J/cm Grade Count:188
 0.224238 - 5338.47 J/cm
@Temperature -40.0 - -18.0 °C
Average value: 1.50 J/cm Grade Count:33
Izod Impact, Unnotched 0.300 - 5340 J/cmAverage value: 0.451 J/cm Grade Count:9
 3.30 - 5338.47 J/cm
@Temperature -18.0 - -18.0 °C
Average value: 3.30 J/cm Grade Count:6
Izod Impact, Notched (ISO) 2.77 - 80.1 kJ/m²Average value: 21.5 kJ/m² Grade Count:31
Charpy Impact, Notched 0.200 - 5.00 J/cm²Average value: 0.758 J/cm² Grade Count:53
 0.200 - 0.530 J/cm²
@Temperature -30.0 - -30.0 °C
Average value: 0.413 J/cm² Grade Count:16
Gardner Impact 22.6 - 22.6 JAverage value: 22.6 J Grade Count:3
Tensile Impact Strength 34.0 - 330 kJ/m²Average value: 121 kJ/m² Grade Count:13
 100 - 348.6 kJ/m²
@Temperature -40.0 - -30.0 °C
Average value: 228 kJ/m² Grade Count:10
Falling Dart Impact 31.1839 - 176.257 J
@Temperature -40.0 - -40.0 °C
Average value: 125 J Grade Count:3
Coefficient of Friction 0.0270 - 0.300Average value: 0.136 Grade Count:3
Tensile Creep Modulus, 1 hour 400 - 570 MPaAverage value: 465 MPa Grade Count:4
Tensile Creep Modulus, 1000 hours 270 - 400 MPaAverage value: 318 MPa Grade Count:4
Tear Strength Test 23.5 - 30.0Average value: 28.4 Grade Count:4
Elmendorf Tear Strength, MD 0.600 - 1.60 g/micronAverage value: 0.940 g/micron Grade Count:5
Elmendorf Tear Strength, TD 1.70 - 23.0 g/micronAverage value: 10.5 g/micron Grade Count:5
Dart Drop 1.50 - 2.00 g/micronAverage value: 1.67 g/micron Grade Count:4
Film Tensile Strength at Break, MD 35.6 - 55.0 MPaAverage value: 47.1 MPa Grade Count:5
Film Tensile Strength at Break, TD 20.0 - 50.0 MPaAverage value: 38.5 MPa Grade Count:6
Tangent Modulus 1170 - 1760 MPaAverage value: 1310 MPa Grade Count:7
Hydrostatic Design Basis 6.89476 - 6.89476 MPa
@Temperature 60.0 - 60.0 °C
Average value: 6.89 MPa Grade Count:1
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 1e+05 - 1.00e+17 ohm-cmAverage value: 2.05e+16 ohm-cm Grade Count:12
Surface Resistance 10000 - 1.00e+14 ohmAverage value: 6.00e+13 ohm Grade Count:7
Dielectric Constant 2.25 - 2.40Average value: 2.36 Grade Count:11
Dielectric Strength 19.7 - 150 kV/mmAverage value: 68.3 kV/mm Grade Count:12
Dissipation Factor 0.0000400 - 0.00100Average value: 0.000207 Grade Count:11
Comparative Tracking Index 600 VAverage value: 600 V Grade Count:4
 
Thermal PropertiesOriginal ValueComments
CTE, linear 20.0 - 165 µm/m-°CAverage value: 120 µm/m-°C Grade Count:18
Melting Point 118 - 137 °CAverage value: 131 °C Grade Count:114
Crystallization Temperature 108 - 120 °CAverage value: 115 °C Grade Count:30
Deflection Temperature at 0.46 MPa (66 psi) 42.8 - 93.3 °CAverage value: 72.9 °C Grade Count:156
Deflection Temperature at 1.8 MPa (264 psi) 32.2 - 86.1 °CAverage value: 50.3 °C Grade Count:48
Vicat Softening Point 64.0 - 194 °CAverage value: 121 °C Grade Count:312
Brittleness Temperature -180 - 76.0 °CAverage value: -73.1 °C Grade Count:161
Flammability, UL94 HBGrade Count:16
Oxygen Index 17.0 %Average value: 17.0 % Grade Count:4
 
Optical PropertiesOriginal ValueComments
Yellow Index -1.00 - 4.00 %Average value: 1.98 % Grade Count:25
 
Processing PropertiesOriginal ValueComments
Processing Temperature 82.2 - 280 °CAverage value: 214 °C Grade Count:33
Nozzle Temperature 160 - 275 °CAverage value: 241 °C Grade Count:26
Melt Temperature 130 - 280 °CAverage value: 221 °C Grade Count:66
Mold Temperature 5.00 - 65.6 °CAverage value: 23.2 °C Grade Count:13
Injection Pressure 2.76 - 103 MPaAverage value: 26.5 MPa Grade Count:4

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Low Density Polyethylene (LDPE), Molded
Overview of materials for Polypropylene, Molded
Overview of materials for High Density Polyethylene (HDPE), Extruded
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Molded
Overview of materials for High Density Polyethylene (HDPE), Ultra High Molecular Weight

O4000 / 78275

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.