MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Möller Medical PolySkin 78 M NanoCoating
Categories: Ceramic; Glass; Glass Ceramic; Other Engineering Material; Ceramic/Metallic Coating

Material Notes: Decorative coating in "metallic look," hardening at room temperature up to 80°C.

Information provided by Möller Medical, Member of CENTROTEC Group

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Thickness 3.00 - 10.0 microns0.118 - 0.394 mil
 
Mechanical PropertiesMetricEnglishComments
Taber Abrasion, mg/1000 Cycles 4444CS17 friction disc with 500g load; DIN 53754
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 200 °C392 °F
 
Processing PropertiesMetricEnglishComments
Processing Temperature 25.0 - 80.0 °C77.0 - 176 °FHardening Temperature
 
Descriptive Properties
Applicable SubstrateABSwith restrictions
 Aluminum
 Brass
 Copper
 Glass
 Nylonwith restrictions
 PMMAwith restrictions
 Polycarbonatewith restrictions
 Stainless Steel
Contact Angle to Water [deg]78
Cupping Test [mm]8.4DIN EN ISO 1520
Non-Applicable SubstrateTubes int. dia. 0.1-10 mm
Pendulum Dampening Test [sec]160-180DIN EN ISO 1522

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Mo-Sci Corporation GL 1738 Glass-ceramic
Möller Medical NanoSkin 92 NanoCoating
Borosilicate Glass
Accuratus MACOR Machinable Glass Ceramic

CMOLL15 / 1636

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.