MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Kingfa HIPS-5197 High Impact Polystyrene
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene, Impact Modified

Material Notes:
    Features:
  • UL 94 HB @ 1.6mm
  • Excellent balance properties
  • High mechanical strength
  • Good heat stability
  • Color tailor-made for clients

    Applications:
  • Injection molding
  • Gas assistant molding
  • TV & Audio housing
  • Electric and electrical cabinet

Information Provided by Kingfa Sci. & Tech. Co., Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.04 g/cc
@Temperature 23.0 °C
ASTM D792
Linear Mold Shrinkage 0.0040 - 0.0060 cm/cm
@Temperature 23.0 °C
ASTM D955
Melt Flow 11 g/10 min
@Load 5.00 kg,
Temperature 200 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 24.0 MPa50mm/min; ASTM D638
Elongation at Break 30 %50mm/min; ASTM D638
Flexural Strength 38.0 MPa2mm/min; ASTM D790
Flexural Modulus 2150 MPa2mm/min; ASTM D790
Izod Impact, Notched 90.0 J/m
@Thickness 3.20 mm,
Temperature 23.0 °C
ASTM D256
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+16 ohm-cmASTM D257
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 78.0 °C
@Thickness 6.40 mm
ASTM D648
Flammability, UL94 HB
@Thickness 1.60 mm
 HB
@Thickness 3.20 mm
 
Processing PropertiesOriginal ValueComments
Processing Temperature <= 250 °C
Rear Barrel Temperature 182 - 205 °CStart Point: 190°C
Middle Barrel Temperature 205 - 230 °CStart Point: 215°C
Front Barrel Temperature 215 - 240 °CStart Point: 225°C
Melt Temperature 220 - 245 °CStart Point: 230°C
Mold Temperature 30.0 - 60.0 °CStart Point: 50°C
Drying Temperature 70.0 °C
@Time 7200 sec
Pre-dry
Back Pressure 5.00 - 15.0 MPa
 
Descriptive Properties
Injection SpeedSlow to Moderate

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LG Chemical 60HR HIPS
INEOS Styrolution PS 495N HIPS
KKPC Kuhmo HI 425 General Purpose HIPS
Americas Styrenics Styron® 425 High Impact Polystyrene
Versalis Edistir N 1840 Polystyrene

PKINGF090 / 104349

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.