Purell HP372P is a polypropylene homopolymer with a gamma – ray stabilizing additivation for use in injection molding applications. Purell HP372P exhibits a high fluidity and very good transparency. Purell HP372P is primarily designed for empty disposable three – part syringes which are not to be supplied in the same package as the medication itself and for other medical applications. Applications: Healthcare Applications, SyringesInformation provided by LyondellBasell. |