MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

Epoxy Technology EPO-TEK® TD1001 Thermally Conductive Epoxy
Categories: Polymer; Thermoset; Epoxy; Epoxy, Thermally Conductive

Material Notes: Product Description: EPO-TEK® TD1001 is a single component, thermally conductive, electrically insulating epoxy designed for low stress semiconductor and electronics packaging.

Advantages & Application Notes:

  • Low Tg, several weeks of pot-life and low modulus are a few of its traits.
  • It is particularly suitable for bonding ferrite cores in power device plastic packaging.
  • Excellent adhesion to PCBs, ceramics, most metals and lead frames.
  • Suggested Applications:
    • Semiconductor:
      • IC packaging on lead frame or FR4 PCB, accepting Epoxy Molding Compound plastic SMD encapsulation.
      • Low stress on large die attach > 500 mil x 500 mil.
    • Electronics:
      • Bonding Cu and Al heat sinks.
      • Staking SMDs to PCBs and other substrates.
    • Optics:
      • LED die attach.
      • White color after cure is attractive for LED, x-ray scintillator, and opto-coupler circuits.
      • Heat sinking laser diode packages.
      • Fiber optic component packaging and assembly.
  • Its smooth and creamy viscosity enables high speed dispensing processes; however, its thixotropic nature allows for screen printing techniques as well.

Information Provided by Epoxy Technology

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.20 g/cc1.20 g/cc
Particle Size <= 20 µm<= 20 µm
Viscosity 10000 - 22000 cP
@Temperature 23.0 °C
10000 - 22000 cP
@Temperature 73.4 °F
5 rpm
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8585
Tensile Modulus 1.98 GPa287 ksiStorage
Shear Strength >= 13.8 MPa>= 2000 psiLap
 >= 35.2 MPa>= 5100 psiDie
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 2.00e+13 ohm-cm>= 2.00e+13 ohm-cm
Dielectric Constant 3.12
@Frequency 1000 Hz
3.12
@Frequency 1000 Hz
Dissipation Factor 0.010
@Frequency 1000 Hz
0.010
@Frequency 1000 Hz
 
Thermal PropertiesMetricEnglishComments
CTE, linear 57.0 µm/m-°C31.7 µin/in-°FBelow Tg
 213 µm/m-°C118 µin/in-°FAbove Tg
Thermal Conductivity 0.770 W/m-K5.34 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 225 °C437 °FContinuous
 325 °C617 °FIntermittent
Minimum Service Temperature, Air -55.0 °C-67.0 °FContinuous
 -55.0 °C-67.0 °FIntermittent
Glass Transition Temp, Tg >= 40.0 °C>= 104 °FDynamic Cure 20—200°C /ISO 25 Min; Ramp 10—200°C @ 20°C/Min
Decomposition Temperature 436 °C817 °FDegradation Temperature
 
Processing PropertiesMetricEnglishComments
Cure Time 60.0 min
@Temperature 125 °C
1.00 hour
@Temperature 257 °F
Minimum Bond Line
Pot Life 40320 min40320 min
Shelf Life 12.0 Month
@Temperature -40.0 °C
12.0 Month
@Temperature -40.0 °F
 
Descriptive Properties
ColorWhite
ConsistencySmooth paste
Number of ComponentsSingle
Thixotropic Index4.1
Weight Loss<0.05%200°C
 0.14%250°C
 0.44%300°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Aluminum 6061-T6; 6061-T651
Aluminum 5052-H32
Epoxy Technology EPO-TEK® 920 Thermally Conductive Epoxy
Epoxy Technology EPO-TEK® H73 Thermally Conductive, Electrically Insulating Epoxy
Epoxy Technology EPO-TEK® 930 Thermally Conductive Epoxy

PPOXYT101 / 141140

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.