MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Oxford Polymers Oxnilon 6-60GF(DRY) PA6, 60% Glass Fiber Reinforced, Dry
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 60% Glass Fiber Filled

Material Notes: Product Description: Glass Fiber (60% Reinforced), Nylon 6 injection molding grade

Processing and Delivery Form: Pellets and Injection Molding

Additives: Release Agents, Lubricants and Heat Stabilizers

Special Characteristics: Colors Available

Information provided by Oxford Polymers

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.65 g/ccASTM D792
Water Absorption at Saturation 4.5 %ASTM D570
Linear Mold Shrinkage, Flow 0.0020 in/in
@Thickness 3.17 mm
ASTM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 35000 psiASTM D638
Elongation at Break 1.0 %ASTM D638
Flexural Strength 52000 psiASTM D790
Flexural Modulus 2.35e+6 psiASTM D790
Izod Impact, Notched 4.00 ft-lb/in
@Thickness 3.17 mm
ASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 414 °FUnannealed; ASTM D648
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 500 - 550 °F
Middle Barrel Temperature 520 - 570 °F
Front Barrel Temperature 535 - 585 °F
Nozzle Temperature 535 - 585 °F
Melt Temperature 520 - 570 °F
Mold Temperature 150 - 255 °F
Drying Temperature 190 °F
Dry Time 4.00 - 6.00 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Washington Penn Homopolymer Polypropylene 40% Glass Reinforced
Plastcom SLOVAMID 6 GF 60 Polyamide 6, 60% Glass Fiber
Oxford Polymers 30GF 30% Glass Fiber Reinforced Polybutylene Terephthalate (PBT)
Overview of materials for Polyphthalamide (PPA), 50% Glass Fiber Reinforced
Avient Edgetek® PPX-40GF/000 Chemically Coupled Polypropylene - 40% Glass Fiber

POXF006 / 178436

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.