MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Astralloy 140 ksi High Strength Quenched and Tempered, Fine Grained Structural Steel
Categories: Metal; Ferrous Metal; Alloy Steel

Material Notes: Astralloy 140 ksi is a fine-grained, general structural steel that yields a minimum tensile strength of 140 ksi (960 MPa). This high-strength alloy plate achieves its mechanical properties by being water quenched and tempered. This structural alloy provides the opportunity to reduce component weight by offering a high strength to weight ratio along with improved ductility. It is formable and weldable when following good shop practice and has a service temperature which ranges from -50°F (-46°C) to 800°F. Astralloy 140 ksi is optimal for use in mining equipment, forestry (427°C) equipment, construction equipment, structural steel works, raw material handling, quarries, shredders, crushers, forestry equipment, cranes, buckets, blades, bridges, shears, booms, hoists, and transport trailers. Each manufacturing mill has its own proprietary chemical composition and heat-treating process.

Information provided by Astralloy, a Nucor Company.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 270 - 310270 - 310
Tensile Strength 979 - 1150 MPa142000 - 167000 psi
Tensile Strength, Yield 965 MPa140000 psi
Bend Radius, Minimum  3.0 t
@Diameter >=50.8 mm
3.0 t
@Diameter >=2.00 in
Transverse; Cold Forming
 4.0 t
@Diameter >=50.8 mm
4.0 t
@Diameter >=2.00 in
Longitudinal; Cold Forming
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 427 °C800 °F
Minimum Service Temperature, Air -45.6 °C-50.0 °F
 
Component Elements PropertiesMetricEnglishComments
Carbon, C <= 0.25 %<= 0.25 %
Chromium, Cr <= 1.25 %<= 1.25 %
Iron, Fe >= 93.3 %>= 93.3 %As Balance
Manganese, Mn <= 1.7 %<= 1.7 %
Molybdenum, Mo <= 0.70 %<= 0.70 %
Nickel, Ni <= 2.0 %<= 2.0 %
Phosphorus, P <= 0.025 %<= 0.025 %
Silicon, Si <= 0.80 %<= 0.80 %
Sulfur, S <= 0.010 %<= 0.010 %
 
Descriptive Properties
Carbon Equivalent<2.0"-0.62
 >2.0"-0.77

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
International Mold Steel DC53 General-Purpose Cold Work Die and Mold Steel
Aluminum, Al
Lithium, Li
Aluminum 3110 Composition Spec
AISI 1030 Steel, water quenched from 870°C (1600°F), 540°C (1000°F) temper, 25 mm (1 in.) round

NNUCOR910 / 233184

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.