MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ExxonMobil LD 33021.07 Low Density Polyethylene Resin
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE)

Material Notes: Product Description: ExxonMobil™ LD 33021.07 resin is a high flow LDPE homopolymer designed to provide good processability. It is suitable for use in making color concentrates and injection molded articles.

Availability: Latin America, North America and South America

Additive:

  • Antiblock: No
  • Slip: No
  • Thermal Stabilizer: Yes
Applications:
  • Caps
  • Closures
  • Compounding
  • Food Packaging Containers
  • Houseware Articles
  • Injection Molding
  • Masterbatch Base Resin

Information provided by ExxonMobil

Key Words: LDPE LD 506.07
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.921 g/ccExxonMobil method
Melt Flow 33 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 91
@Time 15.0 sec
ASTM D2240
Hardness, Shore D 47
@Time 15.0 sec
ASTM D2240
Tensile Strength at Break 1400 psiASTM D638
Tensile Strength, Yield 1900 psiASTM D638
Elongation at Break 94.0 %ASTM D638
Elongation at Yield 50 %ASTM D638
Flexural Modulus, 1% Secant 35000 psiASTM D790
Dart Drop, Total Energy 6.30 ft-lb
@Temperature -40.0 °C
ASTM D3763
 12.0 ft-lb
@Temperature 22.8 °C
ASTM D3763
 
Thermal PropertiesOriginal ValueComments
Melting Point 230 °FPeak Melting Point; ExxonMobil method
Vicat Softening Point 194 °FASTM D1525

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Chevron Phillips Marlex® KN 226 LDPE Injection Molding Resin
ExxonMobil LD 26019.LN Low Density Polyethylene Resin
Chevron Phillips Marlex® 1412 Injection Molding Resin
Braskem PB 608 LDPE Injection Molding Polyethylene
ExxonMobil LD 40022.LI Low Density Polyethylene Resin

PEX99234 / 175470

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.