MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Denka STYROL MW1 Polystyrene  (discontinued **)
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene, Molded, Unreinforced

Material Notes: "DENKA SYTROL MW" is a well-balanced polystyrene (PS) resin, with a high tensile strength as well as good moldability. Overturning the traditional understanding that PS resin is "hard and brittle," this products applications have been expanded to include large packaging cases (and the like), advancing the world of PS resin, and becoming a synonym for ultra-strong PS.

Applications

  • Recording media-related items like CD jewel cases, and videotape or audiocassette cases, etc.
  • Refrigerator trays
  • Pet cages
  • Miscellaneous goods/toys
  • Food packaging, etc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.05 g/ccISO 1183
Melt Flow 1.9 g/10 min
@Load 5.00 kg,
Temperature 200 °C
ASTM D1238
 1.9 g/10 min
@Load 5.00 kg,
Temperature 200 °C
ISO 1133
Spiral Flow 30.5 cm200°C; DENKA method
 42.5 cm240°C; DENKA method
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 77ISO 2039-2
Tensile Strength at Break 46.0 MPaISO 527-2
Elongation at Break <= 3.0 %ISO 527-2
Flexural Strength 51.0 MPaASTM D790
 101 MPaISO 178
Flexural Modulus 3.30 GPaISO 178
Izod Impact, Notched 18.0 J/m
@Temperature 23.0 °C
ASTM D256
Charpy Impact, Notched 0.300 J/cm²
@Temperature 23.0 °C
ISO 179-2
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 72.0 °CISO 75-2
Vicat Softening Point 92.0 °C50N; ISO 306
Flammability, UL94 HB
@Thickness 1.50 mm
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 210 - 240 °CH-3
Middle Barrel Temperature 200 - 230 °CH-2
Front Barrel Temperature 190 - 210 °CH-1
Nozzle Temperature 210 - 240 °C
Mold Temperature 38.0 - 60.0 °C
Injection Pressure 5000 - 30000 psi
Back Pressure 1000 - 4000 psi
 
Descriptive Properties
Falling Weight Test, g/cm50/37

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Aclo Accucomp Polystyrene HS0600L High Impact
American Polymers API 375 Polystyrene
American Polymers API 550 Polystyrene
Chevron Phillips EA3025 Crystal Polystyrene
American Polymers API 505 HF Polystyrene

PDENK000 / 29664

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.