MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Nouryon Promotor D N,N-Diethylacetoacetamide
Categories: Other Engineering Material

Material Notes: Promotor D is a promoter for cobalt-accelerated cure systems using ketone peroxides at ambient and elevated temperatures.

CAS number: 2235-46-3

EINECS/ELINCS No.: 218-792-3

Applications: Promotor D, is a promoter which can be used to increase the reactivity of ketone peroxide/cobalt accelerator based cure systems in a wide variety of unsaturated polyester resins. Promotor D can effectively be used in standard ortho- and iso phthalic acid based polyester resins, Bisphenol A/fumarate resins and vinylester resins. Promotor D can, in vinyl resins, also be used to increase the reactivity of the cure system Trigonox 239/cobalt accelerator and Butanox LPT/ cobalt accelerator. Promotor D can be used in these resins as a substitute for the promoter N,N-Dimethylaniline. In comparison with N,N-Dimethylaniline Promotor D is a low toxic compound.It does not give a yellow to brown discoloration of the cured UP resin part as it is usually observed when aromatic amines are used as promoter.

Information provided by Nouryon

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.994 g/cc
 
Processing PropertiesOriginal ValueComments
Shelf Life 9.00 Month
 
Descriptive Properties
AppearanceClear yellow to reddish brown
Assay= 97.0 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PNOURY861 / 286384

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.