MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

RTP Company RTP 150 UV  Polypropylene (PP) Flame Retardant - Living Hinge Grade - UV Stable  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Flame Retardant

Material Notes: Flame Retardant - Living Hinge Grade - UV Stable

Comments:

  • Flame Retardant
  • Living Hinge Grade
  • UV Stabilized

Unless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.

Information provided by RTP Company.


Data for this product has not been recently verified, please contact RTP Company for more information before specifying this grade.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.25 g/cc1.25 g/ccASTM D792
Water Absorption 0.030 %0.030 %24 hours at 23°C; ASTM D570
Linear Mold Shrinkage  0.012 cm/cm
@Thickness 3.17 mm
0.012 in/in
@Thickness 0.125 in
ASTM D955
 0.016 cm/cm
@Thickness 6.35 mm
0.016 in/in
@Thickness 0.250 in
ASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 23.4 MPa3400 psiASTM D638
Elongation at Break 40 %40 %ASTM D638
Modulus of Elasticity 1.72 GPa250 ksiASTM D638
Flexural Yield Strength 34.5 MPa5000 psiASTM D790
Flexural Modulus 1.45 GPa210 ksiASTM D790
Izod Impact, Notched 0.320 J/cm
@Thickness 3.17 mm
0.600 ft-lb/in
@Thickness 0.125 in
ASTM D256
Izod Impact, Unnotched 5.34 J/cm
@Thickness 3.17 mm
10.0 ft-lb/in
@Thickness 0.125 in
ASTM D256
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 1.00e+16 ohm-cm1.00e+16 ohm-cmASTM D257
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 55.8 µm/m-°C
@Temperature 20.0 °C
31.0 µin/in-°F
@Temperature 68.0 °F
ASTM D696
Thermal Conductivity 0.303 W/m-K2.10 BTU-in/hr-ft²-°FThrough-plane; ASTM C177
Deflection Temperature at 0.46 MPa (66 psi) 113 °C235 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 65.6 °C150 °FASTM D648
Flammability, UL94 V-0
@Thickness 1.59 mm
V-0
@Thickness 0.0625 in
Per testing by RTP Company; ASTM D3801
 
Processing PropertiesMetricEnglishComments
Processing Temperature 193 - 227 °C380 - 440 °F
Mold Temperature 32.2 - 65.6 °C90.0 - 150 °F
Injection Pressure 68.9 - 103 MPa10000 - 15000 psi
 
Descriptive Properties
ColorNatural/Black

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Techmer ES Statiblend® PP FR BK
Techmer ES HiFill FR® PP CO FR HS
Techmer ES HiFill FR® PP CO E FR
RTP Company RTP 150 HI LF  Polypropylene (PP) Flame Retardant - Living Hinge Grade - High Impact - Low Flow
Avient Edgetek® PP-1000 HI FR Polypropylene Copolymer

PR3218 / 62486

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.